Suppr超能文献

双重应用型全酸蚀黏结剂的薄型树脂涂层可提高间接修复体用树脂水门汀的牙本质黏结强度。

Thin resin coating by dual-application of all-in-one adhesives improves dentin bond strength of resin cements for indirect restorations.

机构信息

Cariology and Operative Dentistry, Department of Restorative Sciences, Graduate School of Medical and Dental Sciences, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tokyo 113-8549, Japan.

出版信息

Dent Mater J. 2010 Oct;29(5):615-22. doi: 10.4012/dmj.2009-110. Epub 2010 Sep 1.

Abstract

This study was evaluated the tensile bond strength (TBS) of resin cements to bovine dentin resin-coated with all-in-one adhesive systems. Each of the dual-polymerizing resin cements; Link Max, Clearfil Esthetic Cement, Bistite II and Chemiace II were used to bond indirect resin disks to bovine dentin, as control, or coated by single-application or by dual-application of an adhesive system from the same manufacturer; G-Bond, Clearfil Tri-S Bond, Tokuyama Bond Force and Hybrid-Coat (n=10). After 24-hour water storage, TBSs were measured. The fracture pattern and the adhesive interface were observed using an SEM. Dual-application of the adhesive yielded significantly higher TBSs compared to control and single-application groups for all materials (p<0.001). From the limited information of this study, it was concluded that dual-application of all-in-one adhesive systems created a thin coating on dentin, and significantly improved the bond strengths of resin cements.

摘要

本研究评估了全酸蚀自粘接系统处理后牙本质对树脂水门汀粘结强度的影响。使用 Link Max、Clearfil Esthetic Cement、Bistite II 和 Chemiace II 这 4 种双固化树脂水门汀,将间接树脂片粘结于牛牙本质上作为对照组,或者使用同厂家生产的全酸蚀自粘接系统进行单次或双次处理后粘结于牛牙本质上,分别为 G-Bond、Clearfil Tri-S Bond、Tokuyama Bond Force 和 Hybrid-Coat(n=10)。水储存 24 小时后,测量粘结强度。使用 SEM 观察断裂模式和粘结界面。与对照组和单次应用组相比,所有材料的双次应用的粘结强度均显著更高(p<0.001)。本研究的有限信息表明,全酸蚀自粘接系统的双次应用在牙本质上形成了一层薄涂层,显著提高了树脂水门汀的粘结强度。