Département de Chimie, Pavillon J.A. Bombardier, Universite de Montréal, CP 6128, Succursale Centre Ville, Montréal, QC, H3C 3J7, Canada.
J Am Chem Soc. 2010 Nov 10;132(44):15573-9. doi: 10.1021/ja104182w.
Linear copolymers of ethylene and acrylic acid (PEAA) were prepared by catalytic polymerization of ethylene and tert-butyl acrylate followed by hydrolysis of the ester groups. The copolymers contained COOH groups inserted into the crystalline unit cell with formation of intramolecular hydrogen-bonds, as established on the basis of differential scanning calorimetry (DSC), Fourier-transform infrared spectroscopy (FTIR), and X-ray diffraction (XRD) studies. A solvent-exchange protocol, with no added surfactant, converted a solution in tetrahydrofuran of a PEAA sample containing 12 mol % of acrylic acid (AA) into a colloidally stable aqueous suspension of nanoparticles. Transmission electron microscopy (TEM), dynamic light scattering (DLS), and high sensitivity differential scanning calorimetry (HS-DSC) were used to characterize the nanoparticles. They are single crystals of elongated shape with a polar radius of 49 nm (σ = 15 nm) and an equatorial radius of 9 nm (σ = 3 nm) stabilized in aqueous media via carboxylate groups located preferentially on the particle/water interface. The PEAA (AA: 12 mol %) nanoparticles dispersed in aqueous media exhibited a remarkable reversible thermoresponsive behavior upon heating/cooling from 25 to 80 °C.
线性的乙烯和丙烯酸共聚物(PEAA)是通过催化聚合乙烯和叔丁基丙烯酸酯,然后水解酯基制备的。共聚物含有插入结晶单元的 COOH 基团,形成分子内氢键,这是基于差示扫描量热法(DSC)、傅里叶变换红外光谱(FTIR)和 X 射线衍射(XRD)研究确定的。一种溶剂交换方案,无需添加表面活性剂,将含有 12mol%丙烯酸(AA)的 PEAA 样品在四氢呋喃中的溶液转化为胶体稳定的纳米颗粒水悬浮液。透射电子显微镜(TEM)、动态光散射(DLS)和高灵敏度差示扫描量热法(HS-DSC)用于表征纳米颗粒。它们是长形单晶,极性半径为 49nm(σ=15nm),赤道半径为 9nm(σ=3nm),通过优先位于颗粒/水界面上的羧酸根稳定在水介质中。在水溶液中分散的 PEAA(AA:12mol%)纳米颗粒在从 25°C 加热/冷却至 80°C 时表现出显著的可逆热响应行为。