Department of Dental Materials and Prosthodontics, São José dos Campos Dental School, São Paulo State University, São José dos Campos, SP, Brazil.
J Appl Oral Sci. 2010 Sep-Oct;18(5):477-81. doi: 10.1590/s1678-77572010000500008.
The aim of this study was to evaluate the influence of two adhesive systems and the post space region on the degree of conversion of dual resin cement and its bond strength to root dentin.
One three-step etch-and-rinse (All-bond 2, Bisco) and another one-step self-etch (Xeno III, Dentsply) adhesive systems were applied on 20 (n=10) crownless bovine incisors, at 12-mm-deep post space preparation, and a fiber post (DT Light Post, Bisco) was cemented using a dual cure resin cement (Duo-Link, Bisco). Three transverse sections (3 mm) were obtained, being one from each study region (cervical, middle and apical). The degree of conversion of the dual cure resin cement was determined by a micro-Raman spectrometer. The data (%) were submitted to repeated-measures analysis of variance and Tukey's test (p<0.05).
For both groups, the degree of conversion means (%) (All bond 2cervical = 69.3; All bond 2middle = 55.1; All bond 2apical= 56; Xeno IIIcervical = 68.7; Xeno IIImiddle = 68.8; Xeno IIIapical = 54.3) were not significantly different along the post space regions (p<0.05).
Neither the adhesive nor the post space region influenced the degree of conversion of the cement layer.
本研究旨在评估两种粘接系统和根管预备区域对双重固化树脂水门汀的转化率及其与牙本质的粘接强度的影响。
将两种粘接系统(All-bond 2,Bisco,三步酸蚀-冲洗;Xeno III,Dentsply,一步自酸蚀)应用于 20 个无冠牛切牙(n=10),在 12mm 深的根管预备区域内,使用纤维桩(DT Light Post,Bisco),并采用双重固化树脂水门汀(Duo-Link,Bisco)进行粘接。获得三个横向截面(3mm),每个截面来自研究区域(颈、中、根尖)之一。采用显微拉曼光谱仪测定双重固化树脂水门汀的转化率。数据(%)采用重复测量方差分析和 Tukey 检验(p<0.05)。
对于两组,转化率平均值(%)(All bond 2 颈 = 69.3;All bond 2 中 = 55.1;All bond 2 尖 = 56;Xeno III 颈 = 68.7;Xeno III 中 = 68.8;Xeno III 尖 = 54.3)在根管预备区域内无显著差异(p<0.05)。
粘接系统和根管预备区域均不影响水门汀层的转化率。