Suppr超能文献

掺铒(Er(3+))、铒镱(Er(3+)/Yb(3+))和铒铥镱(Er(3+)/Tm(3+)/Yb(3+))的碲酸盐(TeO(2))-氧化锌(ZnO)-氧化钨(WO(3))-二氧化钛(TiO(2))-氧化钠(Na(2)O)玻璃的光谱分析

Spectral analysis of Er(3+)-, Er(3+)/Yb(3+)- and Er(3+)/Tm(3+)/Yb(3+)-doped TeO(2)-ZnO-WO(3)-TiO(2)-Na(2)O glasses.

作者信息

Lakshminarayana G, Qiu Jianrong, Brik M G, Kumar G A, Kityk I V

机构信息

State Key Laboratory of Silicon Materials, Zhejiang University, Hangzhou 310027, People's Republic of China.

出版信息

J Phys Condens Matter. 2008 Sep 17;20(37):375101. doi: 10.1088/0953-8984/20/37/375101. Epub 2008 Aug 12.

Abstract

In this paper, we present the spectroscopic properties of Er(3+)-, Er(3+)/Yb(3+)- and Er(3+)/Tm(3+)/Yb(3+)-doped novel tellurite glasses. From the measured absorption spectra, Judd-Ofelt (JO) intensity parameters (Ω(2), Ω(4) and Ω(6)) have been evaluated for the Er(3+)-doped glass. With 980 nm excitation three strong upconversion emission bands centered at 505, 520 and 630 nm were observed for both Er(3+)- and Er(3+)/Yb(3+)-codoped glasses and the characteristic near-infrared emission bands were spectrally centered at 1.535 µm. The near-infrared spectra of Er(3+)- and Er(3+)/Yb(3+)-doped glasses have shown full width at half-maxima (FWHM) around 100 nm and 120 nm for the erbium [Formula: see text] transition, respectively. The measured maximum decay times of the [Formula: see text] transition (at wavelength 1.535 µm) are about 7.24 ms and 7.68 ms for 1.0Er(3+) and 1.0Er(3+)/ 2Yb(3+) (mol%)-codoped glasses, respectively. The maximum stimulated emission cross sections for the [Formula: see text] transition of Er(3+) and Er(3+)/Yb(3+) are 8.64 × 10(-21) and 6.78 × 10(-21) cm(2). From 1Er(3+)/ 1Tm(3+)/ 2Yb(3+) (mol%)-codoped glass, broad near-infrared emission bands centered at 1510 nm ([Formula: see text]) and 1637 nm ([Formula: see text]) with full width at half-maxima (FWHM) around 52 nm and 60 nm, respectively, were observed. These glasses with broad near-infrared emissions should have potential applications in tunable lasers and broadband optical amplification at low-loss telecommunication windows.

摘要

在本文中,我们展示了掺铒(Er(3+))、铒镱(Er(3+)/Yb(3+))和铒铥镱(Er(3+)/Tm(3+)/Yb(3+))的新型碲酸盐玻璃的光谱特性。根据测得的吸收光谱,已对掺铒玻璃的贾德 - 奥费尔特(JO)强度参数(Ω(2)、Ω(4)和Ω(6))进行了评估。在980 nm激发下,掺铒和铒镱共掺玻璃均观察到三个强上转换发射带,中心波长分别为505、520和630 nm,且特征近红外发射带的光谱中心位于1.535 µm。掺铒和铒镱掺杂玻璃的近红外光谱显示,铒[公式:见原文]跃迁的半高宽(FWHM)分别约为100 nm和120 nm。对于1.0Er(3+)和1.0Er(3+)/2Yb(3+)(摩尔%)共掺玻璃,测得的[公式:见原文]跃迁(波长1.535 µm处)的最大衰减时间分别约为7.24 ms和7.68 ms。铒和铒镱的[公式:见原文]跃迁的最大受激发射截面分别为8.64×10(-21)和6.78×10(-21) cm(2)。从1Er(3+)/1Tm(3+)/2Yb(3+)(摩尔%)共掺玻璃中,观察到分别以1510 nm([公式:见原文])和1637 nm([公式:见原文])为中心的宽近红外发射带,其半高宽(FWHM)分别约为52 nm和60 nm。这些具有宽近红外发射的玻璃在可调谐激光器和低损耗电信窗口的宽带光放大方面应具有潜在应用。