U,S, Forest Service, Forest Products Laboratory, Madison, WI 53726, USA.
Nanoscale Res Lett. 2011 Jun 15;6(1):427. doi: 10.1186/1556-276X-6-427.
Historically most residential wood preservatives were aqueous soluble metal formulations, but recently metals ground to submicron size and dispersed in water to give particulate formulations have gained importance. In this study, the specific role nano-zinc oxide (ZnO) particle size and leach resistance plays in termite mortality resulting from exposure to particulate ZnO-treated wood was investigated. Southern yellow pine (SYP) sapwood impregnated with three concentrations of two particle sizes (30 and 70 nm) of ZnO were compared to wood treated with soluble zinc sulphate (ZnSO4) preservative for leach resistance and termite resistance. Less than four percent leached from the particulate nano-ZnO-treated specimens, while 13 to 25% of the zinc sulphate leached from the soluble treated wood. Nano-ZnO was essentially non-leachable from wood treated with 5% formulation for the 30-nm particle size. In a no-choice laboratory test, eastern subterranean termites (Reticulitermes flavipes) consumed less than 10% of the leached nano-ZnO-treated wood with 93 to 100% mortality in all treatment concentrations. In contrast, termites consumed 10 to 12% of the leached ZnSO4-treated wood, but with lower mortality: 29% in the 1% treatment group and less than 10% (5 and 8%, respectively) in the group of wood blocks treated with 2.5 and 5.0% ZnSO4. We conclude that termites were repelled from consuming wood treated with nano-ZnO, but when consumed it was more toxic to eastern subterranean termites than wood treated with the soluble metal oxide formulation. There were no differences in leaching or termite mortality between the two particle sizes of nano-ZnO.
从历史上看,大多数住宅木材防腐剂都是水溶性金属制剂,但最近,粒径达到亚微米级并分散在水中的金属得到了广泛应用。本研究旨在探讨纳米氧化锌(ZnO)颗粒大小和抗浸出性在粉状 ZnO 处理木材对白蚁致死作用中的具体作用。南方黄松(SYP)边材用两种粒径(30nm 和 70nm)的三种浓度 ZnO 浸渍,与用可溶性硫酸锌(ZnSO4)防腐剂处理的木材进行抗浸出性和抗白蚁性比较。从粉状纳米 ZnO 处理的标本中浸出的锌不到 4%,而可溶性处理木材中浸出的锌为 13%至 25%。粒径为 30nm 的 5%配方处理的木材中,纳米 ZnO 基本不溶出。在无选择的实验室试验中,东部地下白蚁(Reticulitermes flavipes)消耗的浸出纳米 ZnO 处理木材不到 10%,所有处理浓度的死亡率均为 93%至 100%。相比之下,白蚁消耗了 10%至 12%的浸出 ZnSO4 处理木材,但死亡率较低:1%处理组为 29%,2.5%和 5.0% ZnSO4 处理组的木材块死亡率分别低于 10%和 8%。我们得出的结论是,白蚁排斥消耗用纳米 ZnO 处理的木材,但当消耗时,它对东部地下白蚁的毒性比用可溶性金属氧化物制剂处理的木材更大。两种粒径的纳米 ZnO 在浸出和白蚁死亡率方面没有差异。