The purpose of this study was to evaluate and compare the force levels of aesthetic Ni-Ti wires to regular Ni-Ti wires of the same dimension and evaluate their mechanical properties. Aesthetic and regular maxillary superelastic Ni-Ti wires (0.016 × 0.022) from four different manufacturers (G&H Wire Company, TP Orthodontics, GAC International, and Ortho Organizers) were selected and grouped I-IV. The loading and unloading values were compared using a three-point bending test. The unloading end values were also recorded to evaluate the recovery of archwires after each deflection. The unloading values were recorded at 0.5, 1.5, and 2.5 mm after loading deflections of 1, 2, and 3 mm, respectively. Cross-sectional scanning electron microscopy was used to assess the coating thickness of aesthetic wires. The results, statistically analysed, showed a significant decrease in force values for the aesthetic wires in groups I, III, and IV (P < 0.001) as compared to regular Ni-Ti wires of the same dimension from the same manufacturer. There was no significant difference in force values for group II wires. A statistically significant decrease in force values of epoxy-coated wires was observed in groups I, III, and IV only. This is of obvious clinical significance during wire selection. The group II coated wires, however, exhibited forces comparable to their regular Ni-ti wires with a difference that was statistically insignificant. The end values of aesthetic wires showed almost complete recovery for groups I, II, and III after 2 and 3 mm deflections.
本研究旨在评估和比较相同尺寸的美学镍钛丝和常规镍钛丝的力水平,并评估它们的机械性能。从四个不同制造商(G&H 丝公司、TP 正畸、GAC 国际和 Ortho Organizers)选择并分组 I-IV 的美学和常规上颌超弹性镍钛丝(0.016×0.022)。使用三点弯曲试验比较加载和卸载值。还记录卸载端值,以评估每个挠度后弓丝的恢复情况。在分别加载 1、2 和 3mm 挠度后,在 0.5、1.5 和 2.5mm 处记录卸载值。使用横截面扫描电子显微镜评估美学丝的涂层厚度。经统计学分析,与同一制造商的相同尺寸的常规镍钛丝相比,I、III 和 IV 组的美学丝的力值显著降低(P<0.001)。II 组丝的力值没有差异。仅在 I、III 和 IV 组观察到环氧涂层丝的力值有统计学意义的降低。这在选择丝时具有明显的临床意义。然而,涂层 II 组丝的力值与常规镍钛丝相当,差异无统计学意义。在 2 和 3mm 挠度后,I、II 和 III 组的美学丝的末端值显示出几乎完全恢复。