da Silva Marta Proto, Barceleiro Marcos Oliveira, Dias Katia Regina Hostilio Cervantes, Zanin Fatima
Department of Operative Dentistry, School of Dentistry, Rio de Janeiro State University, Rio De Janeiro, Brazil.
Gen Dent. 2011 May-Jun;59(3):e96-100.
Dentinal surfaces prepared with an Er:YAG laser have distinctly different characteristics compared to those prepared with conventional instruments. The objective of this study was to evaluate the shear bond strength of a total-etch adhesive system and a self-etch adhesive system to dentin, prepared conventionally or with an Er:YAG laser. Specimens that were prepared with a diamond bur and treated with the total-etch adhesive showed the highest mean bond strength, followed by specimens prepared with the laser and treated with the total-etch adhesive, specimens prepared with a diamond bur and treated with the self-etch adhesive, and specimens prepared with the laser and treated with the self-etch adhesive, but there were no differences among the groups (P > 0.05). These data indicate that the tested adhesive systems promote similar shear bond strengths, whether the dentin is prepared with a diamond bur or an Er:YAG laser, and that an Er:YAG laser is a suitable cavity preparation method that promotes an adequate surface for a posterior adhesive procedure.
与使用传统器械制备的牙本质表面相比,用铒激光(Er:YAG激光)制备的牙本质表面具有明显不同的特性。本研究的目的是评估全酸蚀粘结系统和自酸蚀粘结系统与传统制备或用Er:YAG激光制备的牙本质之间的剪切粘结强度。用金刚砂车针制备并经全酸蚀粘结剂处理的试件显示出最高的平均粘结强度,其次是用激光制备并经全酸蚀粘结剂处理的试件、用金刚砂车针制备并经自酸蚀粘结剂处理的试件以及用激光制备并经自酸蚀粘结剂处理的试件,但各组之间无差异(P>0.05)。这些数据表明,无论牙本质是用金刚砂车针还是Er:YAG激光制备,所测试的粘结系统均能促进相似的剪切粘结强度,并且Er:YAG激光是一种合适的窝洞制备方法,可为后牙粘结操作提供足够的表面。