三种不同介质中金属陶瓷合金的离子释放。

Ion release from metal-ceramic alloys in three different media.

机构信息

Ankara Education and Research Hospital, Ministry of Health, Sukriye mh. 06340, Ulucanlar, Ankara, Turkey.

出版信息

Dent Mater J. 2011;30(5):598-610. doi: 10.4012/dmj.2011-031. Epub 2011 Sep 23.

Abstract

The aim of this in vitro study was to assess the effect of pH changes on ion release of metal-ceramic dental casting alloys. Samples from four commercially available alloys (Wirobond C, Wiron 99, Rematitan CP-Ti grade 1, and PontoStar) were prepared and polished. Ion release of alloys subjected to three different pH media (artificial saliva of pH 2.3, pH 6.5 and 0.9% saline solution of pH 7.3) for periods of 7, 15, 30, and 60 days were assessed by means of atomic absorption spectroscopy. Microscopic changes on surfaces of metallic samples before and after immersion were compared by scanning electron microscopy. ANOVA was used for statistical analysis of results. For all ions, pH and period interactions were statistically significant: highest amount of ion release occurred after 60 days of immersion regardless of pH value. For every alloy, ion release results were highest in artificial saliva of pH 2.3 and lowest in 0.9% saline solution. It was concluded that ion release from alloys was pH-dependent.

摘要

本体外研究旨在评估 pH 值变化对金属陶瓷牙科铸造合金离子释放的影响。从四种市售合金(Wirobond C、Wiron 99、Rematitan CP-Ti 级 1 和 PontoStar)中制备和抛光样品。通过原子吸收光谱法评估了在三种不同 pH 值介质(pH 值为 2.3 的人工唾液、pH 值为 6.5 的人工唾液和 pH 值为 7.3 的 0.9%生理盐水溶液)中浸泡 7、15、30 和 60 天的合金的离子释放情况。通过扫描电子显微镜比较了浸泡前后金属样品表面的微观变化。采用方差分析对结果进行统计学分析。对于所有离子,pH 值和时间的相互作用均具有统计学意义:无论 pH 值如何,浸泡 60 天后离子释放量最高。对于每种合金,在 pH 值为 2.3 的人工唾液中的离子释放结果最高,在 0.9%的生理盐水溶液中的最低。结论是合金的离子释放是 pH 值依赖性的。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验