Dumlupinar University, Faculty of Dentistry, Tavsanli Yolu 10. km, 43270 Kutahya, Turkey.
Dent Mater J. 2012 Feb 3;31(1):68-75. Epub 2012 Jan 21.
This study evaluated the radiopacity of different resin-based luting materials and compared the results to human and bovine dental hard tissues. Disc specimens (N=130, n=10 per group) (diameter: 6 mm, thickness: 1 mm) were prepared from 10 resin-based and 3 conventional luting cements. Human canine dentin (n=10), bovine enamel (n=10), bovine dentin (n=10) and Aluminium (Al) step wedge were used as references. The optical density values of each material were measured from radiographic images using a transmission densitometer. Al step wedge thickness and optical density values were plotted and equivalent Al thickness values were determined for radiopacity measurements of each material. The radiopacity values of conventional cements and two resin luting materials (Rely X Unicem and Variolink II), were significantly higher than that of bovine enamel that could be preferred for restorations cemented on enamel. Since all examined resin-based luting materials showed radiopacity values equivalent to or greater than that of human and bovine dentin, they could be considered suitable for the restorations cemented on dentin.
本研究评估了不同树脂基水门汀的射线可透性,并将结果与人牙和牛牙的硬组织进行了比较。从 10 种树脂基和 3 种传统水门汀中制备了直径为 6mm、厚度为 1mm 的圆盘试件(N=130,每组 10 个)。用人犬牙本质(n=10)、牛牙釉质(n=10)、牛牙本质(n=10)和铝(Al)步阶楔形物作为参考。使用透射密度计从射线照片中测量每种材料的光密度值。绘制 Al 步阶楔形物的厚度和光密度值,并确定每个材料射线可透性测量的等效 Al 厚度值。传统水门汀和两种树脂水门汀(Rely X Unicem 和 Variolink II)的射线可透性明显高于牛牙釉质,可优先用于釉质粘结修复。由于所有检查的树脂基水门汀的射线可透性值等于或大于人牙和牛牙本质,因此它们可被认为适用于牙本质粘结修复。