体内使用树脂基复合充填材料治疗后未刺激全唾液中单体的检测与定量分析。

Detection and quantification of monomers in unstimulated whole saliva after treatment with resin-based composite fillings in vivo.

作者信息

Michelsen Vibeke B, Kopperud Hilde B M, Lygre Gunvor B, Björkman Lars, Jensen Einar, Kleven Inger S, Svahn Johanna, Lygre Henning

机构信息

Department of Clinical Dentistry, University of Tromsø, Tromsø, Norway.

出版信息

Eur J Oral Sci. 2012 Feb;120(1):89-95. doi: 10.1111/j.1600-0722.2011.00897.x. Epub 2012 Jan 25.

Abstract

Resin-based dental restorative materials contain allergenic methacrylate monomers, which may be released into saliva after restorative treatment. Monomers from resin-based composite materials have been demonstrated in saliva in vitro; however, studies analyzing saliva after restorative therapy are scarce. The aim of this study was to quantify methacrylate monomers in saliva after treatment with a resin-based composite filling material. Saliva was collected from 10 patients at four start points--before treatment, and 10 min, 24 h, and 7 d after treatment--and analysed by combined chromatography/mass spectrometry. The monomers bisphenol-A diglycidyl methacrylate (Bis-GMA), 2-hydroxyethyl methacrylate (HEMA), and urethane dimethacrylate (UDMA) were detected and quantified in the samples collected shortly (10 min) after treatment. The amounts detected ranged from 0.028 to 9.65 μg ml(-1) for Bis-GMA, from 0.015 to 0.19 μg ml(-1) for HEMA, and from 0.004 to 1.2 μg ml(-1) for UDMA. Triethyleneglycol dimethacrylate (TEGDMA) was detected in four of the samples. Ethoxylated bisphenol-A dimethacrylate (Bis-EMA) was not detected. Monomers were not detected in saliva samples collected before treatment, or 24 h or 7 d after treatment, with the exception of one sample, 24 h after treatment, in which HEMA was detected. In conclusion, monomers from the investigated resin-based composite and adhesive system were present in saliva shortly after treatment. One week after treatment, no monomers could be detected in patients' saliva samples.

摘要

树脂基牙科修复材料含有致敏性甲基丙烯酸酯单体,修复治疗后这些单体可能会释放到唾液中。树脂基复合材料中的单体已在体外唾液中得到证实;然而,分析修复治疗后唾液的研究却很少。本研究的目的是量化使用树脂基复合填充材料治疗后唾液中的甲基丙烯酸酯单体。在四个起始时间点从10名患者收集唾液——治疗前、治疗后10分钟、24小时和7天——并通过色谱/质谱联用进行分析。在治疗后不久(10分钟)收集的样本中检测并定量了双酚A二缩水甘油甲基丙烯酸酯(Bis-GMA)、甲基丙烯酸2-羟乙酯(HEMA)和二甲基丙烯酸聚氨酯(UDMA)单体。检测到的Bis-GMA含量范围为0.028至9.65μg/ml,HEMA为0.015至0.19μg/ml,UDMA为0.004至1.2μg/ml。在四个样本中检测到了三乙二醇二甲基丙烯酸酯(TEGDMA)。未检测到乙氧基化双酚A二甲基丙烯酸酯(Bis-EMA)。在治疗前或治疗后24小时或7天收集的唾液样本中未检测到单体,但有一个治疗后24小时的样本检测到了HEMA除外。总之,在所研究的树脂基复合材料和粘结系统中的单体在治疗后不久存在于唾液中。治疗一周后,在患者的唾液样本中未检测到单体。