Pofale A D, Deo S V
Department, Visvesvaraya National Institute of Technology, Nagpur, Maharashtra -440 010, India.
J Environ Sci Eng. 2010 Oct;52(4):373-8.
The use of fly ash as a replacement of sand has a great potential to benefit our society in terms of reducing demand of natural sand, reducing environmental problems, conserving energy and reducing landfill area requirement. This paper presents an approach to increase the utilization of fly ash and conserve scarcely available natural sand for sustainable development. The experimental investigation by the inclusion of fly ash as a partial replacement of sand as compared to control cement mortar mixes indicated 50% to 100% increase in the compressive strength of mortar at 91 days. Replacement of 50% sand with fly ash can save about 0.4 m3 sand. Comparison of cost per N/mm2 compressive strength has shown about 40% to 60% saving in cost. Based on the experimental results, correlations are developed for finding out the compressive strength and cost at 28 and 91 days. Sand was replaced with 10% to 50% of fly ash by weight and 0.5, 0.55, 0.6 and 0.65 W/C ratios were used. Flow test performed for mortar revealed that as the percentage replacement of sand with the fly ash increased the flow of the mortar decreased. It was also observed that wet and dry densities were more than the control mortar for 10% & 20% replacement of sand with fly ash but for higher replacement percentage density reduced marginally.
使用粉煤灰替代沙子在减少天然砂需求、减少环境问题、节约能源和减少填埋场面积需求方面具有巨大潜力,能够造福社会。本文提出了一种提高粉煤灰利用率并节约稀缺天然砂以实现可持续发展的方法。与对照水泥砂浆混合物相比,通过将粉煤灰作为部分沙子替代品进行的实验研究表明,在91天时砂浆的抗压强度提高了50%至100%。用粉煤灰替代50%的沙子可节省约0.4立方米的沙子。每N/mm²抗压强度的成本比较显示成本节省了约40%至60%。基于实验结果,建立了用于确定28天和91天时抗压强度和成本的相关性。按重量用10%至50%的粉煤灰替代沙子,并使用0.5、0.55、0.6和0.65的水灰比。对砂浆进行的流动试验表明,随着粉煤灰替代沙子百分比的增加,砂浆的流动性降低。还观察到,用粉煤灰替代10%和20%的沙子时,湿密度和干密度高于对照砂浆,但对于更高的替代百分比,密度略有降低。