Suppr超能文献

新型硅胶溶胶-凝胶被动采样器用于监测水系统中的汞。

Novel silica sol-gel passive sampler for mercury monitoring in aqueous systems.

机构信息

Chemistry Department, Trent University, 1600 West Bank Drive, Peterborough, ON, Canada K9J 7B8.

出版信息

Chemosphere. 2013 Jan;90(2):323-8. doi: 10.1016/j.chemosphere.2012.07.022. Epub 2012 Aug 11.

Abstract

A novel passive sampler for mercury monitoring was prepared using organosilica sol-gel materials. It comprises a binding layer with thiol groups for mercury complexation and a porous diffusive layer through which mercury can diffuse and arrive at the binding layer. Our study demonstrated that this new sampler follows the principle of passive sampling. The mass of mercury accumulated in the binding layer depends linearly on the mercury concentration in solution, the sampling rate and the exposure time. A typical sol-gel sampler is characterized by a diffusive layer of 1.2 μm, in which mercury ions diffuse with a coefficient of D=0.09×10(-6) cm(2) s(-1), resulting in an uptake R(s) of 8.8 mL h(-1). The capacity for mercury uptake is approximately 0.64 μg cm(-2). Mercury diffusion and binding in the passive sampler are independent of the type of mercury-chloride complex, which potentially opens the door to use this device for mercury monitoring in a wide range of natural waters.

摘要

一种新型的用于汞监测的被动采样器,使用有机硅溶胶-凝胶材料制备。它包括一个带有硫醇基团的结合层,用于汞的络合,以及一个多孔的扩散层,汞可以通过该扩散层扩散到结合层。我们的研究表明,这种新的采样器遵循被动采样的原理。结合层中积累的汞的质量与溶液中的汞浓度、采样速率和暴露时间呈线性关系。典型的溶胶-凝胶采样器的扩散层的厚度为 1.2μm,其中汞离子以扩散系数 D=0.09×10(-6)cm(2)s(-1)的速度扩散,导致吸收率 R(s)为 8.8mL h(-1)。汞的吸收容量约为 0.64μgcm(-2)。汞在被动采样器中的扩散和结合与氯化汞络合物的类型无关,这为在广泛的天然水中使用该装置进行汞监测开辟了可能性。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验