三磷酸钙溶解-沉淀反应前驱物溶解度对形成的羟基磷灰石力学性能的影响。

Effect of precursor's solubility on the mechanical property of hydroxyapatite formed by dissolution-precipitation reaction of tricalcium phosphate.

机构信息

Department of Biomaterials, Faculty of Dental Science, Kyushu University, 3-1-1 Maidashi, Higashi-ku, Fukuoka 812-8582, Japan.

出版信息

Dent Mater J. 2012;31(6):995-1000.

Abstract

The effect of the solubility of the precursors, alpha tricalcium phosphate (α-TCP) and beta tricalcium phosphate (β-TCP) on the mechanical strength of hydroxyapatite (HAp) bone substitute was investigated. Uniaxially pressed block starting from these precursors were treated hydrothermally with 1 mol/L of ammonia solution at 200°C for various durations. XRD analysis revealed that α-TCP block took 3 h whereas β-TCP block took 240 h for complete transformation to HAp. The porosity of HAp obtained from β-TCP block was found to be lower than that of HAp from α-TCP block. Diametral tensile strength of HAp from β-TCP block showed a significantly higher value than that of HAp from α-TCP block. It is therefore concluded that solubility of precursor affects the mechanical strength of the HAp block.

摘要

研究了前体α-磷酸三钙(α-TCP)和β-磷酸三钙(β-TCP)的溶解度对羟基磷灰石(HAp)骨替代物机械强度的影响。从这些前体出发,通过单轴压制制备块状物,然后将其在 200°C 的 1mol/L 氨水溶液中进行水热处理,处理时间不同。XRD 分析表明,α-TCP 块需要 3 小时,而β-TCP 块则需要 240 小时才能完全转化为 HAp。从β-TCP 块获得的 HAp 的孔隙率被发现低于从α-TCP 块获得的 HAp。从β-TCP 块获得的 HAp 的直径拉伸强度明显高于从α-TCP 块获得的 HAp。因此,可以得出结论,前体的溶解度会影响 HAp 块的机械强度。

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验