Due to an increasing scientific interest in MR-imaging of carious lesions and teeth, an accurate signal characterization of dental restoration materials is necessary for optimization of MR sequence protocols and evaluation of material degradation. Therefore, signal yield and relaxation behavior of common dental restoration materials in comparison to those of dentine of extracted human teeth were assessed in vitro by ultrashort echo time (UTE) sequences.
Eighteen material samples and dentine of two freshly extracted human teeth were investigated on a 3T whole-body clinical MR-scanner. Transverse (T2*) and longitudinal relaxation times (T1) were quantified using a recently published modified Ernst equation that takes relevant in-pulse relaxation effects into account.
All investigated samples could be successfully visualized but maximum signal yield was highly variable between samples. T1-values of the investigated dental restoration materials ranged between 28 and 365 ms, whereas T2*-values ranged between 96 and 917 μs. In contrast, T1-values of dentine (T1=545 ms±299 ms) were higher, while T2*-values (T2*=478 μs±271 μs) showed similar values.
Dental restoration materials and dentine of extracted human teeth can be visualized by UTE sequences and show a broad range of signal yield and relaxation times.
由于人们对龋病和牙齿的磁共振成像越来越感兴趣,因此需要准确地对牙科修复材料的信号进行特征描述,以优化磁共振序列方案并评估材料的降解情况。因此,通过超短回波时间(UTE)序列,对常见牙科修复材料与从两颗刚拔出的人牙中获得的牙本质的信号产率和弛豫行为进行了体外评估。
在 3T 全身临床磁共振扫描仪上,对 18 种材料样本和两颗刚拔出的人牙的牙本质进行了研究。使用最近发表的一种经过改进的 Ernst 方程来定量评估横向(T2*)和纵向弛豫时间(T1),该方程考虑了相关的脉冲内弛豫效应。
所有被调查的样本都可以成功地被可视化,但样本之间的最大信号产率差异很大。所研究的牙科修复材料的 T1 值在 28 到 365 毫秒之间,而 T2* 值在 96 到 917 微秒之间。相比之下,牙本质的 T1 值(T1=545 毫秒±299 毫秒)较高,而 T2* 值(T2*=478 微秒±271 微秒)则相似。
UTE 序列可对牙科修复材料和人牙牙本质进行可视化,且显示出广泛的信号产率和弛豫时间范围。