Sieck B, Takagi S, Chow L C
American Dental Association Health Foundation, Paffenbarger Research Center, National Institute of Standards and Technology, Gaithersburg, Maryland 20899.
J Dent Res. 1990 Jun;69(6):1261-5. doi: 10.1177/00220345900690060701.
The amounts of loosely-bound fluoride (F) deposited on human enamel by two topical F treatments were measured with use of a constant-composition F washing method. Enamel biopsies conducted before treatment and after the washing were used for determination of the firmly-bound F uptake. The results showed that (1) the washing system did not remove F from untreated enamel surface, (2) a four-minute application of an acidulated phosphate fluoride (APF) gel deposited 27.2 (2.4) (mean, S.E.) micrograms of loosely-bound F per cm2 of enamel surface and 186 (111) ppm of firmly-bound F in the outer 10 microns of enamel, and (3) a four-minute application of a pH-2.1 dicalcium phosphate dihydrate (DCPD)-forming solution followed by APF produced 44.9 (3.1) micrograms/cm2 of loosely-bound F and 1280 (354) ppm of firmly-bound F in the outer 10 microns of enamel. The results showed that the DCPD pre-treatment effectively enhanced the enamel reactivity with F, so that the DCPD-APF treated enamel acquired greater amounts of both loosely-bound F and firmly-bound F than did samples treated with APF alone.
采用恒定成分氟冲洗法测量了两种局部用氟处理剂沉积在人牙釉质上的松散结合氟(F)的量。治疗前和冲洗后的牙釉质活检样本用于测定牢固结合的氟摄取量。结果表明:(1)冲洗系统未从未处理的牙釉质表面去除氟;(2)4分钟的酸化磷酸氟(APF)凝胶处理在每平方厘米牙釉质表面沉积了27.2(2.4)(平均值,标准误)微克的松散结合氟,在牙釉质外层10微米中沉积了186(111)ppm的牢固结合氟;(3)4分钟的pH值为2.1的二水磷酸二钙(DCPD)形成溶液处理后再用APF处理,在牙釉质外层10微米中产生了44.9(3.1)微克/平方厘米的松散结合氟和1280(354)ppm的牢固结合氟。结果表明,DCPD预处理有效地增强了牙釉质与氟的反应性,因此,与仅用APF处理的样本相比,DCPD-APF处理的牙釉质获得了更多的松散结合氟和牢固结合氟。