Institute of Bioengineering and Information Technology Materials, Tongji University, Shanghai, 200092, China.
J Mater Sci Mater Med. 2013 Oct;24(10):2391-403. doi: 10.1007/s10856-013-4996-0. Epub 2013 Jul 3.
Borate bioactive glass-based composites have been attracting interest recently as an osteoconductive carrier material for local antibiotic delivery. In the present study, composites composed of borate bioactive glass particles bonded with a chitosan matrix were prepared and evaluated in vitro as a carrier for gentamicin sulfate. The bioactivity, degradation, drug release profile, and compressive strength of the composite carrier system were studied as a function of immersion time in phosphate-buffered saline at 37 °C. The cytocompatibility of the gentamicin sulfate-loaded composite carrier was evaluated using assays of cell proliferation and alkaline phosphatase activity of osteogenic MC3T3-E1 cells. Sustained release of gentamicin sulfate occurred over ~28 days in PBS, while the bioactive glass converted continuously to hydroxyapatite. The compressive strength of the composite loaded with gentamicin sulfate decreased from the as-fabricated value of 24 ± 3 MPa to ~8 MPa after immersion for 14 days in PBS. Extracts of the soluble ionic products of the borate glass/chitosan composites enhanced the proliferation and alkaline phosphatase activity of MC3T3-E1 cells. These results indicate that the gentamicin sulfate-loaded composite composed of chitosan-bonded borate bioactive glass particles could be useful clinically as an osteoconductive carrier material for treating bone infection.
硼酸盐生物活性玻璃基复合材料作为局部抗生素递送的骨传导载体材料,近来受到关注。本研究制备了由硼酸盐生物活性玻璃颗粒与壳聚糖基质结合而成的复合材料,并将其作为硫酸庆大霉素的载体进行了体外评估。研究了复合载体系统在 37°C 的磷酸盐缓冲液中浸泡时间的函数的生物活性、降解、药物释放曲线和抗压强度。通过对成骨 MC3T3-E1 细胞增殖和碱性磷酸酶活性的测定,评估了载硫酸庆大霉素复合载体的细胞相容性。在 PBS 中,硫酸庆大霉素持续释放约 28 天,而生物活性玻璃则不断转化为羟基磷灰石。在 PBS 中浸泡 14 天后,载有硫酸庆大霉素的复合材料的抗压强度从初始值 24±3MPa 下降到约 8MPa。硼酸盐玻璃/壳聚糖复合材料的可溶性离子产物提取物增强了 MC3T3-E1 细胞的增殖和碱性磷酸酶活性。这些结果表明,载硫酸庆大霉素的壳聚糖结合硼酸盐生物活性玻璃颗粒复合材料可用作临床治疗骨感染的骨传导载体材料。