与抛光及老化的氧化锆相对的牙釉质磨损。

Enamel wear opposing polished and aged zirconia.

作者信息

Burgess J O, Janyavula S, Lawson N C, Lucas T J, Cakir D

出版信息

Oper Dent. 2014 Mar-Apr;39(2):189-94. doi: 10.2341/12-345-L. Epub 2013 Jul 12.

Abstract

Aging of dental zirconia roughens its surface through low temperature degradation. We hypothesized that age-related roughening of zirconia crowns may cause detrimental wear to the enamel of an opposing tooth. To test our hypothesis, we subjected artificially aged zirconia and reference specimens to simulated mastication in a wear device and measured the wear of an opposing enamel cusp. Additionally, the roughness of the pretest surfaces was measured. The zirconia specimens, artificially aged by autoclave, showed no significant increase in roughness compared to the nonaged specimens. Furthermore, no significant difference in material or opposing enamel wear between the aged and nonaged zirconia was seen. All zirconia specimens showed less material and opposing enamel wear than the enamel to enamel control or veneering porcelain specimens. Scanning electron micrographs showed relatively smooth surfaces of aged and nonaged zirconia following wear testing. The micrographs of the veneering ceramic showed sharp fractured edges and fragments of wear debris. Zirconia may be considered a wear-friendly material for restorations opposing enamel, even after simulated aging.

摘要

牙科氧化锆的老化会通过低温降解使其表面变得粗糙。我们推测,氧化锆牙冠与年龄相关的表面粗糙可能会对相对牙齿的牙釉质造成有害磨损。为了验证我们的推测,我们将人工老化的氧化锆和对照样本置于磨损装置中进行模拟咀嚼,并测量相对牙釉质尖的磨损情况。此外,还测量了测试前表面的粗糙度。通过高压灭菌人工老化的氧化锆样本与未老化样本相比,粗糙度没有显著增加。此外,老化和未老化氧化锆之间在材料或相对牙釉质磨损方面没有显著差异。所有氧化锆样本的材料磨损和相对牙釉质磨损均小于牙釉质对牙釉质对照样本或贴面瓷样本。扫描电子显微镜图像显示,磨损测试后老化和未老化氧化锆的表面相对光滑。贴面陶瓷的显微镜图像显示出尖锐的断裂边缘和磨损碎片。即使经过模拟老化,氧化锆也可被视为一种对相对牙釉质修复友好的材料。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验