Suppr超能文献

流动复合树脂及修复技术对Ⅱ类洞修复体微渗漏的影响。

Influence of flowable composite and restorative technique on microleakage of class II restorations.

作者信息

Hernandes Natália M A P, Catelan Anderson, Soares Giulliana P, Ambrosano Gláucia M B, Lima Débora A N L, Marchi Giselle M, Martins Luís R M, Aguiar Flávio H B

机构信息

Department of Restorative Dentistry, Piracicaba Dental School, University of Campinas, Piracicaba, São Paulo, Brazil.

出版信息

J Investig Clin Dent. 2014 Nov;5(4):283-8. doi: 10.1111/jicd.12058. Epub 2013 Aug 15.

Abstract

AIM

The aim of the present study was to evaluate the microleakage in class II cavities restored with dental composite by varying the thickness of two flowable composite resins and the restorative technique.

METHODS

A total of 130 cavities were prepared on proximal surfaces of bovine teeth and randomly divided in 13 groups. Twelve experimental groups were performed using flowable composite resin as the liner, and they were divided according to the type of flowable composite resin (Filtek Z350 Flow-Z350F and SureFil SDR Flow-SUR), the thickness of the flowable composite (0.5, 1, or 2 mm), and the restorative technique (flowable composite applied at the cavosurface angle or amelodentinal junction) (n = 10). A control group was performed without using a flowable composite. Following restorative procedures and thermocycling, the samples were immersed in Methylene Blue for 2 h, and prepared for analysis in an absorbance spectrophotometer. All results were statistically analyzed (α = 0.05).

RESULTS

There was no significant difference between the flowable composites (P > 0.05). The restorative techniques influenced microleakage and were flowable composite dependent (P ≤ 0.05). The lower thickness of the flowable composite provided less microleakage (P ≤ 0.05).

CONCLUSION

The use a lower thickness of a flowable composite resin provided less microleakage, suggesting a better sealing tooth-restoration interface.

摘要

目的

本研究旨在通过改变两种可流动复合树脂的厚度和修复技术,评估用牙科复合材料修复的II类洞的微渗漏情况。

方法

在牛牙的近中面制备130个洞,并随机分为13组。12个实验组使用可流动复合树脂作为衬层,根据可流动复合树脂的类型(Filtek Z350 Flow-Z350F和SureFil SDR Flow-SUR)、可流动复合树脂的厚度(0.5、1或2毫米)以及修复技术(在洞缘角或釉牙本质界处应用可流动复合树脂)进行分组(n = 10)。设置一个不使用可流动复合树脂的对照组。在进行修复程序和热循环后,将样本浸入亚甲蓝中2小时,并准备在吸光分光光度计中进行分析。所有结果均进行统计学分析(α = 0.05)。

结果

可流动复合树脂之间无显著差异(P > 0.05)。修复技术影响微渗漏,且与可流动复合树脂有关(P ≤ 0.05)。可流动复合树脂厚度较低时微渗漏较少(P ≤ 0.05)。

结论

使用较低厚度的可流动复合树脂可减少微渗漏,表明牙齿修复界面的密封效果更好。