Alhodiry W, Lyons M F, Chadwick R G
Eur J Prosthodont Restor Dent. 2014 Mar;22(1):20-3.
This study evaluated the effect of contamination with saliva and blood on the bi-axial flexural strength and setting time of pure gray Portland cement and Biodentine (Septodont, Allington, UK). A one-way ANOVA showed that contamination caused no significant difference between the cements in bi-axial flexural strength (P> 0.05). However there was a significant difference in setting time (P<O.001), with Portland cement taking longer than Biodentine, regardless of the contaminant, and contamination with blood increased the setting time of both materials. Biodentine was similar in strength to Portland cement, but had a shorter setting time for both contaminated and non-contaminated samples.
本研究评估了唾液和血液污染对纯灰色波特兰水泥及碧兰麻(Septodont公司,英国阿灵顿)的双轴弯曲强度和凝固时间的影响。单向方差分析表明,污染对两种水泥的双轴弯曲强度没有显著差异(P>0.05)。然而,在凝固时间上存在显著差异(P<0.001),无论污染物是什么,波特兰水泥的凝固时间都比碧兰麻长,并且血液污染会增加两种材料的凝固时间。碧兰麻的强度与波特兰水泥相似,但对于污染和未污染的样品,其凝固时间都较短。