与不可吸收材料钛相比,评估两种镁合金作为可降解植入材料在兔体内的生物相容性。

Evaluation of the biocompatibility of two magnesium alloys as degradable implant materials in comparison to titanium as non-resorbable material in the rabbit.

作者信息

Hampp Carolin, Angrisani Nina, Reifenrath Janin, Bormann Dirk, Seitz Jan-Marten, Meyer-Lindenberg Andrea

机构信息

Small Animal Clinic, University of Veterinary Medicine Hanover, Bünteweg 9, 30559 Hanover, Germany.

Small Animal Clinic, University of Veterinary Medicine Hanover, Bünteweg 9, 30559 Hanover, Germany.

出版信息

Mater Sci Eng C Mater Biol Appl. 2013 Jan 1;33(1):317-26. doi: 10.1016/j.msec.2012.08.046. Epub 2012 Sep 5.

Abstract

The aim of this study is to compare the biocompatibility of the two magnesium based alloys LAE442 and LANd442 with that of titanium. For this purpose, cylindrical implants were introduced into the medullary cavity of rabbit's tibiae for 4 and 8 weeks. Animals without any implant served as a control. In the follow-up, clinical, X-ray and μCT-investigations were performed to evaluate the reactions of the bone towards the implanted materials. After euthanasia, ex vivo μCT- and histological investigations were performed to verify the results of the in vivo tests. It could be shown that all materials induce changes in the bone. Whereas LANd442 caused the most pronounced reactions, such as increasing bone volume and bone porosity and decreasing bone density, titanium showed the most bone-implant contact by forming trabeculae. The tibiae of rabbits without implants also reacted by forming cavities, it is therefore assumed that the surgery method itself influences the bone.

摘要

本研究的目的是比较两种镁基合金LAE442和LANd442与钛的生物相容性。为此,将圆柱形植入物植入兔胫骨骨髓腔4周和8周。未植入任何植入物的动物作为对照。在随访过程中,进行了临床、X射线和μCT检查,以评估骨对植入材料的反应。安乐死后,进行离体μCT和组织学检查,以验证体内试验的结果。结果表明,所有材料都会引起骨的变化。虽然LANd442引起的反应最为明显,如骨体积增加、骨孔隙率增加和骨密度降低,但钛通过形成小梁显示出最多的骨-植入物接触。未植入植入物的兔子的胫骨也通过形成空洞做出反应,因此推测手术方法本身会影响骨。