通过炎症和骨再生的血浆生物标志物监测镁合金植入物的骨整合和降解情况。

Monitoring osseointegration and degradation of Mg-alloy implants through plasma biomarkers of inflammation and bone regeneration.

作者信息

Mota-Silva Eduarda, Martinez Diana C, Basta Giuseppina, Babboni Serena, Del Turco Serena, Fragnito Davide, Salvadori Stefano, Kusmic Claudia, Riehakainen Leon, Panetta Daniele, Campanella Beatrice, Onor Massimo, Plocinski Tomasz, Swieszkowski Wojciech, Menichetti Luca

机构信息

Institute of Life Sciences, Sant'Anna School of Advanced Studies, Pisa, Italy.

Institute of Clinical Physiology, CNR, San Cataldo Research Area, Pisa, Italy.

出版信息

J Tissue Eng. 2025 May 5;16:20417314241290595. doi: 10.1177/20417314241290595. eCollection 2025 Jan-Dec.

Abstract

Magnesium-degradable implants have excellent mechanical and osteogenic properties for temporary orthopedic use but are underutilized due to insufficient methods to monitor implant osseointegration and tissue healing. This study evaluated the use of circulatory biomarkers to monitor the bilateral implantation of a Mg-alloy in rats' femurs. A total of 16 biomarkers were measured from plasma samples collected at multiple timepoints up to 90 days post-implantation. Mg-alloy, Ti-alloy, and Sham (noncritical bone defect) groups were followed with computed tomography, histological, and SEM-EDX analysis. The Sham group showed higher DKK1, OPG, VEGF, and KIM-1 levels than implanted groups. The Mg-alloy group had delayed bone regeneration due to gas release but demonstrated active regeneration up to 180 days and superior osseointegration. Elevated IL-10 and reduced FGF23 at day 28 correlated with accelerated implant degradation. These results underline the complex interactions between biomaterials and biological systems in orthopedic applications and show the value of circulating markers to follow-up implantation.

摘要

镁可降解植入物在临时骨科应用中具有出色的机械和骨生成特性,但由于监测植入物骨整合和组织愈合的方法不足,其未得到充分利用。本研究评估了循环生物标志物在监测大鼠股骨中镁合金双侧植入方面的应用。在植入后长达90天的多个时间点采集血浆样本,共检测了16种生物标志物。对镁合金组、钛合金组和假手术组(非关键性骨缺损)进行了计算机断层扫描、组织学和扫描电子显微镜-能谱分析。假手术组的DKK1、OPG、VEGF和KIM-1水平高于植入组。镁合金组由于气体释放导致骨再生延迟,但在180天内显示出活跃的再生且骨整合良好。第28天IL-10升高和FGF23降低与植入物降解加速相关。这些结果强调了骨科应用中生物材料与生物系统之间复杂的相互作用,并显示了循环标志物在植入物随访中的价值。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/a634/12056334/122bf28b0089/10.1177_20417314241290595-img2.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验