Suppr超能文献

[CaO-P2O5-MgO-SiO2-CaF系玻璃陶瓷牙种植体在猴体内的临床及组织病理学观察]

[Clinical and histopathological observation of CaO-P2O5-MgO-SiO2-CaF system glass ceramic tooth implants in monkeys].

作者信息

Hongo O, Mukainakano Y, Asano M, Kawanami M, Kato H

出版信息

Nihon Shishubyo Gakkai Kaishi. 1989 Dec;31(4):1119-29. doi: 10.2329/perio.31.1119.

Abstract

The present study was undertaken to determine the biocompatibility of a newly-developed CaO-P2O5-MgO-SiO2-CaF system glass ceramic tooth implant. Two adult male monkeys were selected and 12 weeks after extraction of M1 and P1, 8 glass ceramic teeth were implanted into alveolar bone. At 1 week after implantation, 6 teeth were allowed occlusal function, and 2 teeth were left free from occlusion as control teeth. The implants were observed for 4-12 weeks and examined histopathologically. The results were as follows: 1. Seven implanted teeth were well maintained clinically, and only one tooth was lost after 5 weeks. 2. In histopathological observation, implanted teeth were surrounded by bone, and connected by bonyankylosis. At cervix of dental implant, connective tissue as also attached firmly to implanted tooth surfaces and epithelial attachment was observed. 3. Although these implants were allowed occlusal function at an early stage (1 week after implantation), osteogenesis around implants was not disturbed. These results suggest that the new glass ceramic implant has good biocompatibility and is useful as an implant tooth.

摘要

本研究旨在确定一种新开发的CaO-P2O5-MgO-SiO2-CaF系统玻璃陶瓷牙种植体的生物相容性。选取两只成年雄性猴子,在拔除M1和P1牙12周后,将8颗玻璃陶瓷牙植入牙槽骨。植入后1周,6颗牙进行咬合功能,2颗牙不进行咬合作为对照牙。对种植体进行4至12周的观察,并进行组织病理学检查。结果如下:1. 7颗植入牙临床保存良好,仅1颗牙在5周后脱落。2. 组织病理学观察显示,植入牙被骨组织包围,并通过骨性粘连相连。在牙种植体颈部,结缔组织也牢固附着于植入牙表面,并观察到上皮附着。3. 尽管这些种植体在早期(植入后1周)即进行咬合功能,但种植体周围的成骨并未受到干扰。这些结果表明,新型玻璃陶瓷种植体具有良好的生物相容性,可用作种植牙。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验