To evaluate the effect of different surface pre-treatment methods on the microleakage of self-adhesive flowable composites (SAFCs) in comparison with a conventional flowable composite applied with an etch-and-rinse adhesive system.
One hundred and thirty-five standardised Class V cavities were randomly divided into nine groups: (1) three-step etch-and-rinse adhesive (Optibond FL - Kerr, Orange, USA)/flowable composite (Clearfil Majesty Flow - Kuraray, Tokyo, Japan) (E&Ra/flowC); (2) Fusio Liquid Dentin (Pentron Clinical, Orange, USA); (3) Er:YAG Laser/Fusio Liquid Dentin (Er&Las/Fusio Liquid Dentin); (4) Phosphoric Acid/Fusio Liquid Dentin (PhosA/Fusio Liquid Dentin); (5) Polyacrylic Acid/Fusio Liquid Dentin (PolyA/Fusio Liquid Dentin); (6) Vertise Flow (Kerr, Orange, USA); (7) Er:YAG Laser/Vertise Flow (Er&Las/Vertise Flow); (8) Phosphoric Acid/Vertise Flow (PhosA/Vertise Flow); (9) Polyacrylic Acid/Vertise Flow (PolyA/Vertise Flow). After thermocycling and immersion in a 0.5% basic fuchsin, the restorations were evaluated under a stereomicroscope (n = 30). The data were statistically analysed (α = 0.05).
Both SAFCs showed higher leakage scores than E&Ra/flowC in enamel and dentin (p < 0.05). Vertise Flow showed lower leakage than Fusio Liquid Dentin in dentin (p < 0.05). Pre-phosphoric acid etching reduced the microleakage scores of Fusio Liquid Dentin in both enamel and dentin (p < 0.05), while all surface pre-treatment methods led to a significant reduction in the microleakage scores of Vertise Flow at the enamel margin (p < 0.05).
Pre-etching of enamel and dentin by phosphoric acid may be satisfactory in improving the sealing ability of Fusio Liquid Dentin, while phosphoric acid or polyacrylic acid etching or laser irradiation may be used to improve the adhesion of Vertise Flow to enamel.
与应用酸蚀冲洗粘结系统的传统可流动复合树脂相比,评估不同表面预处理方法对自粘结可流动复合树脂(SAFCs)微渗漏的影响。
135个标准化的V类洞随机分为9组:(1)三步酸蚀冲洗粘结剂(Optibond FL - Kerr,美国奥兰治)/可流动复合树脂(Clearfil Majesty Flow - 可乐丽,日本东京)(E&Ra/flowC);(2)Fusio Liquid Dentin(Pentron Clinical,美国奥兰治);(3)铒钇铝石榴石激光/Fusio Liquid Dentin(Er&Las/Fusio Liquid Dentin);(4)磷酸/Fusio Liquid Dentin(PhosA/Fusio Liquid Dentin);(5)聚丙烯酸/Fusio Liquid Dentin(PolyA/Fusio Liquid Dentin);(6)Vertise Flow(Kerr,美国奥兰治);(7)铒钇铝石榴石激光/Vertise Flow(Er&Las/Vertise Flow);(8)磷酸/Vertise Flow(PhosA/Vertise Flow);(9)聚丙烯酸/Vertise Flow(PolyA/Vertise Flow)。经过热循环并浸泡在0.5%碱性品红中后,在体视显微镜下评估修复体(n = 30)。对数据进行统计学分析(α = 0.05)。
两种SAFCs在釉质和牙本质中的渗漏评分均高于E&Ra/flowC(p < 0.05)。Vertise Flow在牙本质中的渗漏低于Fusio Liquid Dentin(p < 0.05)。磷酸预酸蚀降低了Fusio Liquid Dentin在釉质和牙本质中的微渗漏评分(p < 0.05),而所有表面预处理方法均使Vertise Flow在釉质边缘的微渗漏评分显著降低(p < 0.05)。
磷酸对釉质和牙本质进行预酸蚀可能有助于提高Fusio Liquid Dentin的封闭能力,而磷酸或聚丙烯酸酸蚀或激光照射可用于提高Vertise Flow与釉质的粘结力。