Suppr超能文献

抛光后牙体修复材料的颜色稳定性和表面粗糙度

Color stability and surface roughness of polished anterior restorative materials.

作者信息

Yildiz Esma, Sirin Karaarslan Emine, Simsek Mine, Ozsevik Abdul Semih, Usumez Aslıhan

机构信息

Department of Pediatric Dentistry, Faculty of Dentistry, Akdeniz University.

出版信息

Dent Mater J. 2015;34(5):629-39. doi: 10.4012/dmj.2014-344. Epub 2015 Apr 29.

Abstract

The purpose of this study was to investigate the effects of different finishing-polishing techniques on the color stability and surface roughness of various anterior restorative materials after staining. A composite, a compomer, and a resin-modified glass ionomer were used to prepare 120 specimens. Specimens were divided into subgroups: polishing discs, liquid polishing material, aluminium oxidebonded discs, and control. The specimens were stained in a coffee solution. Color parameters (Lab*) and surface roughness before and after staining were measured. The color was affected by the material type (p<0.05) and finishing-polishing systems (p<0.05). The composite showed the highest color stability; however, the color differences of all groups were visible even to the nonskilled operator. The Ra values did not significantly change after staining for any of the restorative groups (p>0.05). The finishing-polishing systems had an effect on color after storing in staining solution.

摘要

本研究的目的是调查不同的精修-抛光技术对各种前牙修复材料染色后颜色稳定性和表面粗糙度的影响。使用一种复合树脂、一种复合体和一种树脂改性玻璃离子体制作120个样本。样本被分为亚组:抛光盘、液体抛光材料、氧化铝粘结盘和对照组。样本在咖啡溶液中染色。测量染色前后的颜色参数(Lab*)和表面粗糙度。颜色受材料类型(p<0.05)和精修-抛光系统(p<0.05)影响。复合树脂表现出最高的颜色稳定性;然而,即使对于非专业操作人员,所有组的颜色差异也是可见的。对于任何修复组,染色后Ra值均无显著变化(p>0.05)。精修-抛光系统对储存在染色溶液后的颜色有影响。