Siddhapara K S, Shah D V
J Nanosci Nanotechnol. 2014 Aug;14(8):6337-41. doi: 10.1166/jnn.2014.8833.
In this research, we have studied the doping behaviors of three transition metal ion dopants on the crystal phase, particle sizes, XRD patterns, EDAX spectra, and photoreactivity of TiO2 nanoparticles. Test metal ion concentrations ranged from 1% to 4 at.%, we report the growth of [Fe, Co and Mn]xTiO2 nanocrystals prepared by Sol-Gel technique, followed by freeze-drying treatment at -30 °C temperature for 12 hrs. The obtained Gel was thermally treated at different temperature like 200 °C, 400 °C, 600 °C, 800 °C. Thermal gravimetric analysis (TGA) shows that dopant concentration affects thermal decomposition. The photoreactivities of transition metal ion-doped TiO2 nanoparticles under UV irradiation were quantified by the degradation of formaldehyde.
在本研究中,我们研究了三种过渡金属离子掺杂剂对TiO2纳米颗粒的晶相、粒径、XRD图谱、EDAX光谱和光反应性的掺杂行为。测试的金属离子浓度范围为1%至4原子百分比,我们报告了通过溶胶-凝胶技术制备的[Fe、Co和Mn]xTiO2纳米晶体的生长情况,随后在-30°C温度下进行12小时的冷冻干燥处理。所得凝胶在200°C、400°C、600°C、800°C等不同温度下进行热处理。热重分析(TGA)表明掺杂剂浓度会影响热分解。通过甲醛的降解来量化过渡金属离子掺杂的TiO2纳米颗粒在紫外光照射下的光反应性。