用于后牙修复的可流动树脂复合材料的体外磨损情况。

In vitro wear of flowable resin composite for posterior restorations.

作者信息

Shinkai Koichi, Taira Yoshihisa, Suzuki Shiro, Suzuki Masaya

机构信息

Department of Operative Dentistry, The Nippon Dental University School of Life Dentistry at Niigata.

出版信息

Dent Mater J. 2016;35(1):37-44. doi: 10.4012/dmj.2015-080.

Abstract

The purpose of this study was to examine three- and two-body wear values of flowable resin composites for posterior restorations, using a mechanical loading device. The cavities prepared on flattened extracted molars were restored with flowable resin composites (Clearfil Majesty LV: MLV, Estelite Flow Quick: EFQ, Beautifil Flow Plus F00: BFP, and MI Fill: MIF) using accompanying adhesive systems. A universal resin composite (Clearfil Majesty) was used as a control. The specimens were subjected to in vitro three- and two-body wear testing. MLV showed high wear value (three-body: 14.69 µm, two-body: 0.268 mm(3)) compared with other materials tested in both three- and two-body wear tests. BFP showed high three-body wear value (5.78 µm), whereas low two-body wear value (0.008 mm(3)). MIF and EFQ showed equivalent wear values (MIF, three-body: 0.42 µm, two-body: 0.026 mm(3); EFQ, three-body: 1.15 µm, two-body: 0.14 mm(3)) to that of the control in both wear tests.

摘要

本研究的目的是使用机械加载装置,检测用于后牙修复的可流动树脂复合材料的三体和二体磨损值。在磨平的离体磨牙上制备的窝洞,使用配套的粘结系统,用可流动树脂复合材料(Clearfil Majesty LV:MLV、Estelite Flow Quick:EFQ、Beautifil Flow Plus F00:BFP和MI Fill:MIF)进行修复。使用通用树脂复合材料(Clearfil Majesty)作为对照。对标本进行体外三体和二体磨损测试。在三体和二体磨损测试中,与其他测试材料相比,MLV显示出较高的磨损值(三体:14.69 µm,二体:0.268 mm³)。BFP显示出较高的三体磨损值(5.78 µm),而二体磨损值较低(0.008 mm³)。在两项磨损测试中,MIF和EFQ显示出与对照相当的磨损值(MIF,三体:0.42 µm,二体:0.026 mm³;EFQ,三体:1.15 µm,二体:0.14 mm³)。

文献检索

告别复杂PubMed语法,用中文像聊天一样搜索,搜遍4000万医学文献。AI智能推荐,让科研检索更轻松。

立即免费搜索

文件翻译

保留排版,准确专业,支持PDF/Word/PPT等文件格式,支持 12+语言互译。

免费翻译文档

深度研究

AI帮你快速写综述,25分钟生成高质量综述,智能提取关键信息,辅助科研写作。

立即免费体验