Suppr超能文献

使用牙科粘合剂作为树脂复合材料的建模液体。

Use of dental adhesives as modeler liquid of resin composites.

作者信息

Münchow Eliseu Aldrighi, Sedrez-Porto José Augusto, Piva Evandro, Pereira-Cenci Tatiana, Cenci Maximiliano Sergio

机构信息

Graduate Program in Dentistry, School of Dentistry, Federal University of Pelotas, Pelotas, RS 96015-560, Brazil.

Graduate Program in Dentistry, School of Dentistry, Federal University of Pelotas, Pelotas, RS 96015-560, Brazil.

出版信息

Dent Mater. 2016 Apr;32(4):570-7. doi: 10.1016/j.dental.2016.01.002. Epub 2016 Feb 3.

Abstract

OBJECTIVES

Resin adhesives (RA) have been applied between resin composite (RC) increments, but there is no consensus on the impact of this technique on the properties of the final restoration. This study evaluated the effect of the presence of RA between RC layers on physical properties, translucency and long-term color stability of the restorative material.

METHODS

Scotchbond™ Multi-Purpose (bond, 3M ESPE) and Adper™ Single Bond 2 (3M ESPE) were used as RA, and Filtek™ Z350 (3M ESPE) as RC. Specimens containing RA were prepared by applying 3 layers of the adhesive between 4 increments of RC; adhesive-free specimens were also used (control). Tests of water sorption and solubility, mechanical performance (microtensile cohesive strength, flexural strength, and flexural modulus, after immediate and long-term water storage), and translucency and color stability (after immediate and 1, 7, 90, and 180 days of water or wine storage) were performed. Scanning electron microscopy (SEM) images were also taken from the fractured specimens (flexural strength test). Data were analyzed using ANOVA and Tukey test (p<0.05).

RESULTS

Scotchbond (SBMP) showed lower water sorption and solubility than the control (p<0.001), and an overall similar (p≥0.198, immediate tests) or higher (p≤0.019, long-term tests) mechanical performance. SBMP exhibited a rougher cross-sectional surface compared to the other groups. Translucency remained unaltered after 180 days of storage (p≥0.313), except for single bond that had increased translucency with wine storage (p<0.045). After 180 days, all groups changed color (p≤0.002), although more intensively when immersed in wine.

SIGNIFICANCE

The presence of RA within RC increments increased the physical stability of the material, being this effect more evident by using the hydrophobic unfilled adhesive resin (SBMP). This study is the first to show positive results from the use of resin adhesives as modeler liquid of resin composite, which is common in clinical practice.

摘要

目的

树脂黏结剂(RA)已应用于树脂复合材料(RC)各增量层之间,但对于该技术对最终修复体性能的影响尚无共识。本研究评估了RC层间存在RA对修复材料物理性能、半透明度及长期颜色稳定性的影响。

方法

选用Scotchbond™多用途黏结剂(黏结剂,3M ESPE公司)和Adper™单组分黏结剂2(3M ESPE公司)作为RA,Filtek™ Z350(3M ESPE公司)作为RC。含RA的试件通过在4层RC之间涂抹3层黏结剂制备;同时使用无黏结剂试件作为对照。进行了吸水率和溶解率测试、力学性能测试(即刻和长期水储存后的微拉伸内聚强度、弯曲强度和弯曲模量)以及半透明度和颜色稳定性测试(即刻以及水或葡萄酒储存1、7、90和180天后)。还对断裂试件(弯曲强度测试)进行了扫描电子显微镜(SEM)成像。数据采用方差分析和Tukey检验进行分析(p<0.05)。

结果

Scotchbond(SBMP)的吸水率和溶解率低于对照组(p<0.001),力学性能总体相似(即刻测试,p≥0.198)或更高(长期测试,p≤0.019)。与其他组相比,SBMP的横截面表面更粗糙。储存180天后,除单组分黏结剂在葡萄酒储存后半透明度增加外(p<0.045),其他组半透明度保持不变(p≥0.313)。180天后,所有组均发生颜色变化(p≤0.002),但浸泡在葡萄酒中时颜色变化更明显。

意义

RC增量层中存在RA可提高材料的物理稳定性,使用疏水性未填充黏结剂树脂(SBMP)时这种效果更明显。本研究首次表明,在临床实践中常用的将树脂黏结剂用作树脂复合材料的塑形液体可产生积极效果。