Behery Haytham, El-Mowafy Omar, El-Badrawy Wafa, Saleh Belal, Nabih Sameh
Department of Restorative Dentistry, Faculty of Dentistry, University of Toronto, Toronto, Ontario, Canada.
Department of Operative Dentistry, Faculty of Dental Medicine, Al-Azhar University, Cairo, Egypt.
J Esthet Restor Dent. 2016 Mar-Apr;28(2):122-30. doi: 10.1111/jerd.12188. Epub 2016 Feb 19.
This in vitro study compared cuspal deflection of premolars restored with three bulk-fill composite resins to that of incrementally-restored ones with a low-shrinkage silorane-based restorative material.
Forty freshly-extracted intact human upper premolars were used. Reference points at buccal and palatal cusp tips were acid-etched and composite rods were horizontally bonded to them (TPH-Spectra-HV, Dentsply). Two acrylic resin guiding paths were made for each premolar to guide beaks of a digital micrometer used for cuspal deflection measurements. Standardized MOD cavities, 3 mm wide bucco-lingually and 3.5 mm deep, were prepared on each premolar. Prepared teeth were then equally divided into four groups (n = 10) and each group was assigned to one of four composite resin (QuiXX, Dentsply; X-tra fil, Voco; Tetric EvoCeram Bulk Fill, Ivoclar Vivadent; low-shrinkage Filtek LS, 3M/ESPE). Adper Single Bond-Plus, 3M/ESPE was used with all bulk-fill restoratives. LS-System Adhesive, 3M/ESPE was used with Filtek LS. For each prepared premolar, cuspal deflection was measured in microns as the difference between two readings between reference points before and after restoration completion. Means and SDs were calculated and data statistically-analyzed using One-way ANOVA and Tukey's test.
Filtek LS showed the lowest mean cuspal deflection value 6.4(0.84)μm followed by Tetric EvoCeram Bulk Fill 10.1(1.2) μm and X-tra fil 12.4(1.35)μm, while QuiXX showed the highest mean 13(1.05)μm. ANOVA indicated significant difference among mean values of groups (p < 0.001). Tukey's test indicated no significant difference in mean values between QuiXX and X-tra fil (p = 0.637).
Tetric EvoCeram Bulk Fill had significantly lower mean cuspal deflection compared with the two other bulk-fill composite resins tested. Filtek LS had the lowest significant mean cuspal deflection in comparison to all tested bulk-fill restoratives.
The use of Tetric EvoCeram Bulk fill composite resin restorative for class II MOD cavities resulted in reduced cuspal deflection in comparison to the two other bulk-fill composite resins tested. The silorane-based Filtek LS restorative resulted in the least cuspal deflection in comparison to all tested bulk-fill composite restoratives.
本体外研究比较了用三种大块充填复合树脂修复的前磨牙与用低收缩率的基于硅氧烷的修复材料分层修复的前磨牙的牙尖偏斜情况。
使用40颗新鲜拔除的完整人类上颌前磨牙。对颊尖和腭尖的参考点进行酸蚀,并将复合树脂棒水平粘结于其上(TPH-Spectra-HV,登士柏公司)。为每颗前磨牙制作两条丙烯酸树脂导向路径,以引导用于测量牙尖偏斜的数字千分尺的测头。在每颗前磨牙上制备标准化的近中- 牙合面- 远中(MOD)洞形,颊舌径3 mm,洞深3.5 mm。然后将制备好的牙齿平均分为四组(n = 10),每组分别使用四种复合树脂之一(QuiXX,登士柏公司;X-tra fil,VOCO公司;Tetric EvoCeram Bulk Fill,义获嘉伟瓦登特公司;低收缩率的Filtek LS,3M/ESPE公司)。所有大块充填修复材料均使用3M/ESPE公司的Adper Single Bond-Plus粘结剂。Filtek LS使用3M/ESPE公司的LS-System粘结剂。对于每颗制备好的前磨牙,以修复完成前后参考点之间两次读数的差值为牙尖偏斜量,单位为微米。计算均值和标准差,并使用单因素方差分析和Tukey检验对数据进行统计学分析。
Filtek LS的平均牙尖偏斜值最低,为6.4(0.84)μm,其次是Tetric EvoCeram Bulk Fill,为10.1(1.2)μm,X-tra fil为12.4(1.35)μm,而QuiXX的平均值最高,为13(1.05)μm。方差分析表明各组均值之间存在显著差异(p < 0.001)。Tukey检验表明QuiXX和X-tra fil的均值之间无显著差异(p = 0.637)。
与另外两种测试的大块充填复合树脂相比,Tetric EvoCeram Bulk Fill的平均牙尖偏斜显著更低。与所有测试的大块充填修复材料相比,Filtek LS的平均牙尖偏斜最低。