State Key Laboratory of Oil and Gas Reservoir Geology and Exploitation, Southwest Petroleum University, Xindu, Chengdu, Sichuan 610500, PR China.
State Key Laboratory of Oil and Gas Reservoir Geology and Exploitation, Southwest Petroleum University, Xindu, Chengdu, Sichuan 610500, PR China.
Carbohydr Polym. 2016 Aug 20;147:455-463. doi: 10.1016/j.carbpol.2016.04.029. Epub 2016 Apr 8.
pH is an important factor affecting the performance of polymer fluid. The rheological properties of hydroxypropyl guar gum (HPG) base fluid and the structural strength, rheological properties, viscoelastic properties and thixotropy properties of HPG gel depend largely on the pH values. For the base fluid, an apparent viscosity-increasing effect was observed over the pH range from 7 to 11, and the apparent viscosity gradually decreased at pH 11.5-14, exhibiting electrostatic repulsion behavior and steric effects. For the HPG gel, at pH 7-12.5, the gel possessed higher apparent viscosity, higher elastic modulus (G'), lower tanδ (the ratio of the viscous modulus to the elastic modulus) and an "8"-shaped hysteresis loop, indicating stronger gel structure strength and the elastic dominant property. At pH 13-13.5, the gel samples exhibited the transition from a pseudoplastic fluid to a Newtonian fluid, and their viscosity, elastic modulus decreased but tanδ increased with the increase in pH values, exhibiting gradually weakened elastic properties. When the pH was 14, the gel mainly exhibited viscous characteristics.
pH 值是影响聚合物流体性能的一个重要因素。羟丙基胍胶(HPG)基液的流变性以及 HPG 凝胶的结构强度、流变性、黏弹性和触变性在很大程度上取决于 pH 值。对于基液,在 pH 值为 7 至 11 的范围内观察到表观粘度增加的效果,而在 pH 值为 11.5-14 时,表观粘度逐渐降低,表现出静电排斥行为和空间位阻效应。对于 HPG 凝胶,在 pH 值为 7-12.5 时,凝胶具有较高的表观粘度、较高的弹性模量(G')、较低的 tanδ(粘性模量与弹性模量的比值)和“8”字形滞后环,表明凝胶结构强度较强,弹性主导特性。在 pH 值为 13-13.5 时,凝胶样品从假塑性流体转变为牛顿流体,其粘度、弹性模量随着 pH 值的增加而降低,tanδ 增加,表明弹性性能逐渐减弱。当 pH 值为 14 时,凝胶主要表现出粘性特性。