A superior piezoelectric coefficient (d = 570 ± 10 pC N ), the highest value reported to date in potassium-sodium niobate-based ceramics, is obtained in (1-x-y)K Na Nb Sb O BaZrO - Bi K HfO ceramics. This high d value can be ascribed to the co-existence of "nano-scale strain domains" (1-2 nm) and a high density of ferroelectric domain boundaries. Therefore, ternary KNN-based ceramics demonstrate the potential for applications.