Suppr超能文献

不同冠内漂白方法对粘结于漂白牙釉质上的陶瓷托槽剪切粘结强度的影响:一项研究。

Effect of different intracoronal bleaching methods on shear bond strength of ceramic brackets bonded to bleached enamel: An study.

作者信息

Chauhan Vikas, Kumar Piush, Sharma Payal, Shetty Divya

机构信息

Department of Orthodontics and Dentofacial Orthopaedics, I.T.S Centre for Dental Studies and Research, Muradnagar, Ghaziabad, Uttar Pradesh, India.

出版信息

J Orthod Sci. 2017 Jul-Sep;6(3):86-90. doi: 10.4103/jos.JOS_149_16.

Abstract

OBJECTIVE

To investigate the effect of different intracoronal bleaching methods on the shear bond strength and site of failure of ceramic brackets.

MATERIALS AND METHODS

Sixty freshly extracted human maxillary incisors were randomly divided into four groups ( = 15). Endodontic access cavity was prepared and root canals were filled, root fillings were removed 2mm apical to the cementoenamel junction, and a 2-mmthick layer of glass ionomer cement base was applied. Group 1 served as the control. Intracoronal bleaching was performed with 35% carbamide peroxide in group 2, sodium perborate in group 3, and 37.5% hydrogen peroxide in group 4. The teeth were immersed in artificial saliva for 4 weeks before bracket bonding. Ceramic brackets were bonded with composite resin and cured with LED light. After bonding, the shear bond strength of the brackets was tested with a universal testing machine. The site of bond failure was determined by modified ARI (Adhesive Remnant Index).

RESULTS

The highest value of shear bond strength was measured in control group (18.67 ± 1.59 MPa), which was statistically significant from groups 2,3, and 4. There was no significant difference between groups 2 and 4. The lowest shear bond strength was measured in group 3. ARI scores were not significant from each other.

CONCLUSIONS

Intracoronal bleaching significantly affected the shear bond strength of ceramic brackets even after 4 weeks of bleaching. Bleaching with sodium perborate affects shear bond strength more adversely than does bleaching with other agents like hydrogen peroxide and carbamide peroxide.

摘要

目的

探讨不同的冠内漂白方法对陶瓷托槽抗剪粘结强度及粘结失败部位的影响。

材料与方法

将60颗新鲜拔除的人上颌中切牙随机分为四组(每组n = 15)。制备牙髓腔通路并充填根管,在牙骨质牙釉质界根尖方2mm处去除根充物,并应用一层2mm厚的玻璃离子水门汀基底。第1组作为对照组。第2组用35%过氧化脲进行冠内漂白,第3组用过硼酸钠,第4组用37.5%过氧化氢。在粘结托槽前,将牙齿浸泡在人工唾液中4周。用复合树脂粘结陶瓷托槽并用LED光固化。粘结后,用万能试验机测试托槽的抗剪粘结强度。通过改良的ARI(粘结剂残留指数)确定粘结失败部位。

结果

对照组的抗剪粘结强度最高(18.67±1.59MPa),与第2、3、4组相比有统计学意义。第2组和第4组之间无显著差异。第3组的抗剪粘结强度最低。ARI评分彼此之间无显著差异。

结论

即使在漂白4周后,冠内漂白仍显著影响陶瓷托槽的抗剪粘结强度。与过氧化氢和过氧化脲等其他试剂漂白相比,过硼酸钠漂白对抗剪粘结强度的影响更不利。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/9ab1/5508408/093e02cabb81/JOS-6-86-g002.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验