Haralur Satheesh B, Alasabi Asim Nasser A, Al Qahtani Sultan A Abohathrah, Alqahtani Saeed Musleh S
Department of Prosthodontics, College of Dentistry, King Khalid University, Abha.
Intern Dentist, College of Dentistry, King Khalid University, Abha.
Eur J Dent. 2017 Jul-Sep;11(3):380-384. doi: 10.4103/ejd.ejd_280_16.
The objective of this study is to evaluate the effect of irrigating agents on push-out bond strength of resin postcemented with various adhesive systems at different radicular dentin sections.
Sixty single-rooted premolar teeth were root canal treated, subsequently decorated at cementoenamel junction. The endodontic postspace was irrigated with 5.25% sodium hypochlorite (NaOCl) and 17% ethylenediaminetetraacetic acid (EDTA) for Group A ( = 30) and Group B ( = 30), respectively. The sample from each group was subdivided into three groups (10) according to luting protocol of etch-wash, self-etch, and self-adhesive. Individual teeth with cemented resin postsamples were sectioned into coronal, middle, and apical segments. Subsequently, subjected for pushout bond strength test by applying a load at 0.5 mm/min speed. The data were analyzed by three-way analysis of variance and Tukey comparison test at a significant difference level of 0.05.
The coronal section with 5.25% NaOCl irrigation and self-etch luting protocol provided the highest push out strength at 16.282 Mpa. The etch-wash luting protocol in both irrigations showed the lesser bond strength at 8.273 and 8.493 MPa, respectively, in coronal section.
The self-etch adhesive system showed better push out bond strength and 17% EDTA had a negative influence on self-etch bond strength. The coronal sections had highest bond strength in comparison with apical radicular dentin sections.
本研究的目的是评估冲洗剂对在不同牙根牙本质部位用各种粘结系统粘结的树脂桩的推出粘结强度的影响。
60颗单根前磨牙进行根管治疗,随后在牙釉质牙骨质界处进行修整。A组(n = 30)和B组(n = 30)分别用5.25%次氯酸钠(NaOCl)和17%乙二胺四乙酸(EDTA)冲洗根管桩间隙。根据酸蚀冲洗、自酸蚀和自粘结的粘结方案,将每组样本再细分为三组(每组10个)。将粘结有树脂桩样本的单个牙齿切成冠段、中段和根尖段。随后,以0.5 mm/min的速度加载进行推出粘结强度测试。数据采用三因素方差分析和Tukey比较检验进行分析,显著性差异水平为0.05。
在冠段,用5.25% NaOCl冲洗并采用自酸蚀粘结方案时,推出强度最高,为16.282 Mpa。在两种冲洗情况下,酸蚀冲洗粘结方案在冠段的粘结强度较低,分别为8.273 MPa和8.493 MPa。
自酸蚀粘结系统显示出更好的推出粘结强度,17% EDTA对自酸蚀粘结强度有负面影响。与根尖牙本质段相比,冠段的粘结强度最高。