Ohkubo Kei, Kohno Naoki, Yamada Yusuke, Fukuzumi Shunichi
Department of Material and Life Science , Graduate School of Engineering , Osaka University , ALCA , Japan Science and Technology Agency (JST) , Suita , Osaka 565-0871 , Japan . Email:
Chem Sci. 2015 Jan 1;6(1):666-674. doi: 10.1039/c4sc02269f. Epub 2014 Sep 9.
Metal-free photocatalytic hydrogen evolution occurred efficiently in benzene containing single-walled carbon nanotubes under laser irradiation at 532 nm with an extremely high turnover number of 2 000 000 and a high quantum yield of 130%. The rate of hydrogen evolution increased with increasing laser intensity to exhibit a fourth power dependence, suggesting that hydrogen was evolved four-photon processes in which the coupling of two radical anions derived from benzene is the rate-determining step and the benzene radical anion is produced by electron transfer from benzene to the doubly excited state of single-walled carbon nanotubes, which requires two photons. Polymerisation of benzene was induced by the photogenerated CH˙, accompanied by hydrogen evolution, resulting in a leverage effect to increase the quantum yield of hydrogen evolution to well over the 25% expected for the four-photon process. Laser-induced hydrogen evolution also occurred in water containing single-walled carbon nanotubes. In contrast to the case of benzene, water was not oxidized but hydrogen evolution from water was accompanied by the multi-oxidation of single-walled carbon nanotubes. The yield of hydrogen based on one mole of single-walled carbon nanotubes with 1.4 nm diameter and 1-5 mm length was determined to be 2 700 000%, when oxidations of single-walled carbon nanotubes occurred to produce the polyhydroxylated product.
在532nm激光照射下,含单壁碳纳米管的苯中高效发生无金属光催化析氢反应,其周转数极高,达到2000000,量子产率高达130%。析氢速率随激光强度增加而增大,呈现四次方依赖关系,这表明析氢过程为四光子过程,其中苯衍生的两个自由基阴离子的偶联是速率决定步骤,苯自由基阴离子是通过苯向单壁碳纳米管双激发态的电子转移产生的,这需要两个光子。光生CH˙引发苯的聚合反应,同时伴随析氢,从而产生杠杆效应,使析氢量子产率提高到远超过四光子过程预期的25%。含单壁碳纳米管的水中也会发生激光诱导析氢反应。与苯的情况不同,水不会被氧化,但水的析氢伴随着单壁碳纳米管的多次氧化。当单壁碳纳米管发生氧化生成多羟基化产物时,基于1摩尔直径为1.4nm、长度为1 - 5mm的单壁碳纳米管的析氢产率被测定为2700000%。