Am J Dent. 2017 Oct;30(5):279-284.
To comparatively evaluate universal adhesives and two-step self-etch adhesives for enamel bond fatigue durability in self-etch mode.
Three universal adhesives (Clearfil Universal Bond; G-Premio Bond; Scotchbond Universal Adhesive) and three two-step self-etch adhesives (Clearfil SE Bond; Clearfil SE Bond 2; OptiBond XTR) were used. The initial shear bond strength and shear fatigue strength of the adhesive to enamel in self-etch mode were determined.
The initial shear bond strengths of the universal adhesives to enamel in self-etch mode was significantly lower than those of two-step self-etch adhesives and initial shear bond strengths were not influenced by type of adhesive in each adhesive category. The shear fatigue strengths of universal adhesives to enamel in self-etch mode were significantly lower than that of Clearfil SE Bond and Clearfil SE Bond 2, but similar to that OptiBond XTR. Unlike two-step self-etch adhesives, the initial shear bond strength and shear fatigue strength of universal adhesives to enamel in self-etch mode was not influenced by the type of adhesive.
This laboratory study showed that the enamel bond fatigue durability of universal adhesives was lower than Clearfil SE Bond and Clearfil SE Bond 2, similar to Optibond XTR, and was not influenced by type of adhesive, unlike two-step self-etch adhesives.
在自酸蚀模式下,比较通用型粘结剂和两步法自酸蚀粘结剂对牙釉质粘结疲劳耐久性的影响。
使用三种通用型粘结剂(可乐丽通用粘结剂;G-Premio Bond;3M Scotchbond通用粘结剂)和三种两步法自酸蚀粘结剂(可乐丽SE粘结剂;可乐丽SE粘结剂2;OptiBond XTR)。测定了自酸蚀模式下粘结剂与牙釉质的初始剪切粘结强度和剪切疲劳强度。
通用型粘结剂在自酸蚀模式下与牙釉质的初始剪切粘结强度显著低于两步法自酸蚀粘结剂,且每种粘结剂类型中的初始剪切粘结强度不受粘结剂类型的影响。通用型粘结剂在自酸蚀模式下与牙釉质的剪切疲劳强度显著低于可乐丽SE粘结剂和可乐丽SE粘结剂2,但与OptiBond XTR相似。与两步法自酸蚀粘结剂不同,通用型粘结剂在自酸蚀模式下与牙釉质的初始剪切粘结强度和剪切疲劳强度不受粘结剂类型的影响。
本实验室研究表明,通用型粘结剂对牙釉质的粘结疲劳耐久性低于可乐丽SE粘结剂和可乐丽SE粘结剂2,与Optibond XTR相似,且与两步法自酸蚀粘结剂不同,不受粘结剂类型的影响。