El-Shamy Hassan, Sonbul Helal, Alturkestani Najlaa, Tashkandi Abeer, Loomans Bas Ac, Dörfer Christof, El-Badrawy Wafa
Department of Operative Dentistry Faculty of Dentistry, King Abdulaziz University.
Nahda University, Faculty of Dentistry, Conservative Dentistry Department.
Dent Mater J. 2019 Feb 8;38(1):96-100. doi: 10.4012/dmj.2017-279. Epub 2018 Nov 1.
This study investigated the effect of bulk-fill composites on proximal contact tightness (PCT) of composite restorations using different matrix systems. 150/standardized-MO-ivorine cavity preparations were divided into 5 groups; Smart Dentin Replacement (SDR), SonicFill (SF), Tetric EvoCeram Bulk-Fill (TEB), G-ænial Universal Flo (GF) and Tetric EvoCeram (TE). Each group was subdivided into 3 sub-groups (n=10); Dixieland band in Tofflemire retainer, FenderMate and Palodent plus matrix systems. PCT was measured 24 h post-curing using Tooth Pressure Meter. PCT means were calculated and statistically-analyzed using ANOVA and Tukey's post-hoc test (p<0.05). Means and SD of PCT for Tofflemire subgroup were: 1.75(0.13), 3.21(0.1), 3.06(0.19), 2.49(0.21) and 3.18(0.1) for (SDR), (SF), (TEB), (GF) and (TE), respectively. Using FenderMate, values were: 1.87(0.08), 3.35(0.12), 3.17(0.16), 2.64(0.1) and 3.26(0.11) for (SDR), (SF), (TEB), (GF) and (TE), respectively, while with Palodentplus; 3.16(0.17), 4.23(0.11), 4.1(0.1), 3.46(0.17) and 3.98(0.1) for (SDR), (SF), (TEB), (GF) and (TE), respectively. ANOVA revealed significant differences (p<0.05) between all samples except between (SF), (TEB) and (TE) and also significant difference between Palodentplus and two subgroups. Effect of bulk-fill composites on PCT is material dependent. Separation ring is recommended for proper PCT.
本研究调查了使用不同基质系统的大块充填复合树脂对复合树脂修复体邻面接触紧密性(PCT)的影响。将150个标准化的近中-牙合面-象牙色窝洞制备分为5组;智能牙本质替代材料(SDR)、声波充填材料(SF)、Tetric EvoCeram大块充填材料(TEB)、G-ænial通用流动树脂(GF)和Tetric EvoCeram(TE)。每组再细分为3个亚组(n = 10);使用托弗勒米勒固位器中的迪克西兰带环、FenderMate和Palodent plus基质系统。使用牙齿压力计在固化后24小时测量PCT。计算PCT平均值,并使用方差分析和Tukey事后检验进行统计分析(p<0.05)。托弗勒米勒亚组的PCT平均值和标准差分别为:(SDR)组1.75(0.13)、(SF)组3.21(0.1)、(TEB)组3.06(0.19)、(GF)组2.49(0.21)和(TE)组3.18(0.1)。使用FenderMate时,(SDR)、(SF)、(TEB)、(GF)和(TE)组的值分别为:1.87(0.08)、3.35(0.12)、3.17(0.16)、2.64(0.1)和3.26(0.11),而使用Palodentplus时,(SDR)、(SF)、(TEB)、(GF)和(TE)组的值分别为:3.16(0.17)、4.23(0.11)、4.1(0.1)、3.46(0.17)和3.98(0.1)。方差分析显示,除了(SF)、(TEB)和(TE)组之间以及Palodentplus与两个亚组之间存在显著差异外,所有样本之间均存在显著差异(p<0.05)。大块充填复合树脂对PCT的影响取决于材料。建议使用分离环以获得合适的PCT。