Ni/ZnO was prepared by co-precipitation and used as adsorbent for reactive adsorption desulfurization (RADS) of dibenzothiophene. The effect of calcination temperature, precipitate washing solvent, and reduction temperature on the adsorption performance of Ni/ZnO was investigated. It is observed that Ni/ZnO adsorbent calcined at 350 °C, washed with ethanol, and unreduced or reduced at low temperature performed best. By the characterization of BET, XRD, TPR, FTIR, and in situ XAFS, the optimal calcination temperature leads to the small crystallite of NiO and ZnO species. Washing with ethanol enhances the surface area of adsorbent and decreases its particle size. The influence of reduction temperature on the RADS performance is stronger than that of calcination temperature, which is ascribed to high-temperature reduction that makes the adsorbent easier to sinter and form a Ni-Zn alloy. The high RADS activity is a result of the adsorbent pretreatment conditions, which can form small Ni and ZnO particles, and the synergism between precursors.
通过共沉淀法制备了Ni/ZnO,并将其用作二苯并噻吩反应吸附脱硫(RADS)的吸附剂。研究了煅烧温度、沉淀洗涤溶剂和还原温度对Ni/ZnO吸附性能的影响。结果表明,在350℃煅烧、用乙醇洗涤、未还原或低温还原的Ni/ZnO吸附剂性能最佳。通过BET、XRD、TPR、FTIR和原位XAFS表征发现,最佳煅烧温度导致NiO和ZnO物种的微晶较小。用乙醇洗涤可提高吸附剂的比表面积并减小其粒径。还原温度对RADS性能的影响强于煅烧温度,这归因于高温还原使吸附剂更容易烧结并形成Ni-Zn合金。高RADS活性是吸附剂预处理条件的结果,该条件可形成小的Ni和ZnO颗粒以及前驱体之间的协同作用。