玷污层厚度对自粘接修复材料的粘结强度有影响,但与牙本质干燥无关。

Bond Strength of Self-Adhesive Restorative Materials Affected by Smear Layer Thickness but not Dentin Desiccation.

出版信息

J Adhes Dent. 2020;22(1):79-84. doi: 10.3290/j.jad.a43932.

Abstract

PURPOSE

To use shear bond strength (SBS) testing to determine the effect of surface moisture and smear layer thickness on the adhesion of self-adhesive restorative materials and a universal adhesive.

MATERIALS AND METHODS

One single-step self-etch universal adhesive, Prime & Bond Active (PA), was used to bond Ceram.x Spectra ST HV composite resin to dentin and enamel using the self-etching technique. Three commercially available restorative materials and one newly developed material with self-adhesive properties, Activa (A), Fuji II LC(F), Equia Forte (E), and ASAR-MP4 (S), respectively, were also bonded to enamel and dentin prepared moist and dry and to dentin prepared with a thick smear layer. Shear bond testing was performed using an Ultradent bonding apparatus.

RESULTS

The universal adhesive generated the highest SBS to dentin and enamel, followed by the newly developed material. None of the materials tested were significantly affected by the moisture conditions on enamel or dentin. The thickness of smear layer significantly affected SBS to dentin for S, F, and E. However, S and F still exhibited higher shear bond strength to dentin with the thicker smear layer compared to the other self-adhesive materials. Only the universal adhesive in self-etch mode was not affected by the thicker smear layer and maintained significantly higher SBS.

CONCLUSION

None of the materials tested were affected by bonding to overdried dentin or enamel. All of the self-adhesive materials exhibited lower SBS to specimens with a thicker smear layer. The newly developed material ASAR-MP4 compared favorably to the other self-adhesive materials tested under all test conditions.

摘要

目的

使用剪切结合强度(SBS)测试来确定表面水分和玷污层厚度对自粘结修复材料和通用粘结剂粘结的影响。

材料和方法

使用一步法自酸蚀通用粘结剂 Prime & Bond Active(PA),采用自酸蚀技术将 Ceram.x Spectra ST HV 复合树脂粘结到牙本质和釉质上。还将三种市售的修复材料和一种具有自粘结性能的新型材料 Activa(A)、Fuji II LC(F)、Equia Forte(E)和 ASAR-MP4(S)分别粘结到准备湿润和干燥的釉质和牙本质以及准备有厚玷污层的牙本质上。使用 Ultradent 粘结设备进行剪切结合测试。

结果

通用粘结剂在牙本质和釉质上产生的 SBS 最高,其次是新型材料。在釉质或牙本质上,没有任何测试材料受到水分条件的显著影响。玷污层的厚度显著影响 S、F 和 E 在牙本质上的 SBS。然而,与其他自粘结材料相比,S 和 F 仍然在较厚的玷污层上表现出更高的牙本质剪切结合强度。只有自酸蚀模式的通用粘结剂不受较厚玷污层的影响,并保持显著更高的 SBS。

结论

测试的材料在粘结到过度干燥的牙本质或釉质上均不受影响。所有自粘结材料在玷污层较厚的情况下表现出较低的 SBS。新型材料 ASAR-MP4 在所有测试条件下均优于其他测试的自粘结材料。