García-Palacín Marta, Martínez José Ignacio, Paseta Lorena, Deacon Adam, Johnson Timothy, Malankowska Magdalena, Téllez Carlos, Coronas Joaquín
Chemical and Environmental Engineering Department, Instituto de Nanociencia de Aragón (INA) and Instituto de Materiales de Aragón (ICMA), Universidad de Zaragoza-CSIC, 50018 Zaragoza, Spain.
Johnson Matthey Technology Centre, Belais Avenue, Billingham, TS23 1LB, United Kingdom.
ACS Sustain Chem Eng. 2020 Feb 24;8(7):2973-2980. doi: 10.1021/acssuschemeng.9b07593. Epub 2020 Feb 10.
The effect of different deprotonators as well as washing steps and drying procedure on the synthesis of ZIF-8 from the mother liquor was investigated. The morphology, thermal stability, crystallinity, and surface area of the synthesized MOF were investigated. In addition, life-cycle assessment (LCA) or, in other words, eco-balance, was implemented as well. LCA compares the full range of environmental effects associated with the product by evaluating all inputs and outputs of material flows and predicting how such flow will affect the environment. ZIF-8 nanocrystals were synthesized from the recycled mother liquors using NaOH or NHOH thus preserving the main characteristics of the ZIF-8 nanoparticles derived from the initial synthesis. The rest of the characterization methods confirmed the suitability of the synthesis methodology considering the phase purity of the obtained ZIF-8 and nanometer size particles. This procedure enabled us not only to obtain phase pure ZIF-8 but also to substantially decrease the amount of solvent used for washing making it a sustainable process.
研究了不同去质子剂以及洗涤步骤和干燥程序对从母液合成ZIF-8的影响。对合成的金属有机框架(MOF)的形态、热稳定性、结晶度和表面积进行了研究。此外,还进行了生命周期评估(LCA),换句话说,即生态平衡评估。LCA通过评估物质流的所有输入和输出,并预测这种流动将如何影响环境,来比较与产品相关的全方位环境影响。使用NaOH或NHOH从回收的母液中合成ZIF-8纳米晶体,从而保留了初始合成所得ZIF-8纳米颗粒的主要特性。考虑到所获得的ZIF-8的相纯度和纳米尺寸颗粒,其余的表征方法证实了合成方法的适用性。该程序不仅使我们能够获得相纯的ZIF-8,而且还能大幅减少用于洗涤的溶剂量,使其成为一个可持续的过程。