Mikrochim Acta. 2020 Oct 9;187(11):602. doi: 10.1007/s00604-020-04564-5.
A new class of polymeric sorbents based on deep eutectic solvents (DESs) is introduced. These materials are obtained from simple and inexpensive precursors via an energy-efficient process. The primary benefit of these sorbents is that they possess the unique characteristics of DESs and porous materials simultaneously. Moreover, the possibility of tailoring deep eutectic solvents allows designing a specific polymer for a desired analyte, based on its physical and chemical properties. In this work, the deep eutectic solvent of tetrabutylammonium bromide and acrylic acid (1:2 molar ratio) was prepared and then polymerized under solventless condition. The synthesized polymer was characterized by FT-IR spectroscopy, X-ray diffraction (XRD), field emission scanning electron microscopy (SEM), and Brunauer, Emmett and Teller analysis (BET) to evaluate the properties of the sorbent. The poly (TBAB-2AA DES) was applied as a selective sorbent for preconcentration of lead from food and water samples prior to its quantification by flame atomic absorption spectroscopy (FAAS). Variable factors affecting the extraction were optimized, and under the optimum conditions, the calibration plot was linear in the range 5.0-250.0 μg L. The relative standard deviation was (for n = 5) (RSD) < 3%. The limit of detection (LOD) and the enhancement factor were found to be 2.0 μg L and 50, respectively. Finally, the accuracy of the method was assessed by comparison of the results with those obtained by direct determination of lead using inductively coupled plasma mass spectrometry (ICP-MS) and spiked real samples. The obtained recoveries were between 92 and 106%. Graphical abstract.
介绍了一类基于深共熔溶剂(DESs)的新型聚合吸附剂。这些材料是通过节能工艺由简单且廉价的前体制备得到的。这些吸附剂的主要优点是它们同时具有 DESs 和多孔材料的独特特性。此外,深共熔溶剂的可设计性使得能够根据目标分析物的物理和化学性质,设计出特定的聚合物。在这项工作中,制备了四丁基溴化铵和丙烯酸(1:2 摩尔比)的深共熔溶剂,然后在无溶剂条件下聚合。通过傅里叶变换红外光谱(FT-IR)、X 射线衍射(XRD)、场发射扫描电子显微镜(SEM)和 Brunauer、Emmett 和 Teller 分析(BET)对合成的聚合物进行了表征,以评估吸附剂的性能。将聚(TBAB-2AA DES)用作选择性吸附剂,用于食品和水样中铅的预浓缩,然后通过火焰原子吸收光谱法(FAAS)进行定量。优化了影响提取的可变因素,并在最佳条件下,校准曲线在 5.0-250.0μg L 范围内呈线性。相对标准偏差(n=5)(RSD)<3%。检测限(LOD)和增强因子分别为 2.0μg L 和 50。最后,通过与电感耦合等离子体质谱法(ICP-MS)直接测定铅的结果和加标实际样品进行比较,评估了该方法的准确性。回收率在 92%至 106%之间。