Wang Kaipeng, Zhao Lihong, He Beihai
State Key Laboratory of Pulp and Paper Engineering, South China University of Technology, Guangzhou 510000, China.
Polymers (Basel). 2021 May 16;13(10):1607. doi: 10.3390/polym13101607.
Here, we report a non-toxic method for improving the oil-resistant performance of chitosan coated paper by coating the mixture of chitosan and montmorillonite (MMT) instead of coating chitosan solution only. Through combining MMT into the chitosan coatings, the coated paper exhibited a lower air permeability and enhanced oil resistance under a lower coating load. For coated papers C2.5 and C3 by coating 2.5% () and 3% () chitosan without adding MMT in the chitosan coating, the coating load was 3.76 g/m and 3.99 g/m, respectively, and the kit rating values were only 7-8/12. Regarding the sample C2M0.1 coated by the mixed solution containing 2% () chitosan and 0.1% () MMT, its coating load was only 3.65 g/m, the paper permeability after coating was reduced to 0.00507 μm/Pa·s, owing to the filling of MMT into the cellulosic fibers network, and the kit rating reached 9/12. Moreover, C2M0.1 showed improved mechanical properties, whereby its tearing resistance was 5.2% and 6.6% higher than that of the uncoated paper in the machine direction and the cross direction, respectively.
在此,我们报道了一种无毒方法,通过涂布壳聚糖和蒙脱石(MMT)的混合物而非仅涂布壳聚糖溶液来提高壳聚糖涂布纸的耐油性能。通过将MMT混入壳聚糖涂层中,涂布纸在较低的涂布量下表现出较低的透气率和增强的耐油性。对于在壳聚糖涂层中未添加MMT、分别涂布2.5%()和3%()壳聚糖的涂布纸C2.5和C3,涂布量分别为3.76 g/m²和3.99 g/m²,试剂盒评级值仅为7 - 8/12。对于由含有2%()壳聚糖和0.1%()MMT的混合溶液涂布的样品C2M0.1,其涂布量仅为3.65 g/m²,由于MMT填充到纤维素纤维网络中,涂布后纸张的透气率降至0.00507 μm/Pa·s,试剂盒评级达到9/12。此外,C2M0.1的机械性能有所改善,其抗撕裂性在纵向和横向分别比未涂布纸高5.2%和6.6%。