Polymers (Basel). 2021 Sep 13;13(18):3082. doi: 10.3390/polym13183082.
Optimal bond strength between the prefabricated post/dowel to the surrounding dentin is essential. The present study aimed to analyze and compare the effect of three different cement film thicknesses on the pull-out bond strength of three different prefabricated post systems. Extracted natural teeth (N = 90) with similar root dimensions were acquired. Teeth were mounted in resin blocks, endodontically treated, sectioned at cemento-enamel junction, divided into three groups (A: Parapost Fiber Lux plus; B: 3M ESPE Relyx fiber post; and C: Parapost XP), and stored. Uniform post spaces were prepared for the groups (A and C: Length = 8 mm, Width = 1.5 mm; B: Length = 8 mm, Width = 1.6 mm). Each group (N = 30) was further subdivided into three subgroups (n = 10) based on the size (4, 5, and 6) of the post and cemented with resin cement (MultiLink-N, Ivoclar Vivadent). After thermocycling, the specimens were subjected to a pull-out test using a universal testing machine, and tensile force was recorded (MPa). Digital microscopic evaluations were performed for modes of failure. ANOVA and Tukey-HSD tests were used for statistics. Significant differences were observed for each tested material ( = 0.000). The lowest and highest bond strength values were recorded for Group C (Titanium post) and Group A (000), respectively. Multiple comparisons showed significance ( < 0.05) among all the groups, except for space 1 and space 2 ( = 0.316) for Group A. Most of the failures occurred within the cement-dentin and post-cement interface (Adhesive failures, 73.5%). An increase in the luting cement film thickness results in the decrease in pull-out bond strength of prefabricated posts luted with resin cement, irrespective of the type/material/shape of the post. The serrated fiber posts showed the highest pull-out bond strength compared to the smooth surfaced fiber posts or serrated metal posts. Increased pull-out bond strengths were observed when appropriate post space was created with the same sized drill as the post size.
预制桩/桩钉与周围牙本质之间的最佳粘结强度至关重要。本研究旨在分析和比较三种不同粘结剂膜厚度对三种不同预制桩系统拔出粘结强度的影响。获取了牙根尺寸相似的拔除天然牙(N = 90)。将牙齿固定在树脂块中,进行根管治疗,在牙骨质-釉质界处切片,分为三组(A组:Parapost Fiber Lux plus;B组:3M ESPE Relyx纤维桩;C组:Parapost XP)并储存。为各组制备均匀的桩道(A组和C组:长度 = 8 mm,宽度 = 1.5 mm;B组:长度 = 8 mm,宽度 = 1.6 mm)。每组(N = 30)根据桩的尺寸(4、5和6)进一步细分为三个亚组(n = 10),并用树脂粘结剂(MultiLink-N,义获嘉伟瓦登特公司)粘结。热循环后,使用万能试验机对标本进行拔出试验,并记录拉伸力(MPa)。对失效模式进行数字显微镜评估。采用方差分析和Tukey-HSD检验进行统计学分析。每种测试材料均观察到显著差异(P = 0.000)。C组(钛桩)和A组(000)分别记录到最低和最高粘结强度值。多重比较显示,除A组的空间1和空间2(P = 0.316)外,所有组之间均有显著性差异(P < 0.05)。大多数失效发生在粘结剂-牙本质和桩-粘结剂界面(粘结失效,73.5%)。无论桩的类型/材料/形状如何,粘结剂膜厚度的增加都会导致用树脂粘结剂粘结的预制桩拔出粘结强度降低。与光滑表面纤维桩或锯齿状金属桩相比,锯齿状纤维桩显示出最高的拔出粘结强度。当使用与桩尺寸相同的钻头创建合适的桩道时,观察到拔出粘结强度增加。