J Adhes Dent. 2021 Dec 3;23(6):497-503. doi: 10.3290/j.jad.b2288205.
The aim of this clinical trial was to compare a self-adhesive flowable resin composite, a highly filled flowable resin composite used in combination with a universal adhesive applied in self-etch mode, and a conventional flowable resin composite used in combination with a universal adhesive applied using two different application modes in occlusal cavities.
Twenty-eight patients received 114 occlusal restorations. Cavities were divided into four groups: CS: a self-adhering flowable (Constic, DMG); GF: a highly filled flowable (G-ænial Universal Flo, GC) in combination with a universal adhesive applied in self-etch mode (G-Premio Bond, GC); TF-SE: a conventional flowable (Tetric N-Flow, Ivoclar Vivadent) in combination with a universal adhesive (Tetric N-Bond Universal, Ivoclar Vivadent) applied in self-etch mode; TF-ER: a conventional flowable (Tetric N-Flow, Ivoclar Vivadent) in combination with a universal adhesive (Tetric N-Bond Universal, Ivoclar Vivadent) applied in etch&rinse mode. Restorations were scored using modified USPHS criteria. Descriptive statistics were performed using chi-squared tests.
At 24-month evaluations, none of the restorations were lost. The CS group showed significantly higher bravo scores for marginal adaptation than did the other experimental groups (p = 0.024). Significant changes were seen for CS and GF regarding marginal adaptation compared to baseline.
Although the self-adhering flowable resin composite exhibited inferior marginal adaptation compared to the highly filled flowable and conventional flowable resin composites, the restored teeth demonstrated a clinically acceptable performance after 24 months.
本临床试验旨在比较自粘接流动树脂复合材料、高填充流动树脂复合材料与通用自酸蚀粘结剂联合应用于自酸蚀模式、以及传统流动树脂复合材料与通用粘结剂联合应用于两种不同应用模式在咬合面窝洞的情况。
28 名患者共接受了 114 个咬合面修复。将窝洞分为四组:CS 组:自粘接流动树脂复合材料(Constic,DMG);GF 组:高填充流动树脂复合材料(G-ænial Universal Flo,GC)与通用自酸蚀粘结剂联合应用(G-Premio Bond,GC);TF-SE 组:传统流动树脂复合材料(Tetric N-Flow,Ivoclar Vivadent)与通用自酸蚀粘结剂(Tetric N-Bond Universal,Ivoclar Vivadent)联合应用;TF-ER 组:传统流动树脂复合材料(Tetric N-Flow,Ivoclar Vivadent)与通用自酸蚀粘结剂(Tetric N-Bond Universal,Ivoclar Vivadent)联合应用于酸蚀-冲洗模式。使用改良的 USPHS 标准对修复体进行评分。采用卡方检验进行描述性统计分析。
在 24 个月的评估中,没有一个修复体脱落。CS 组的边缘适合性 Bravo 评分明显高于其他实验组(p = 0.024)。与基线相比,CS 和 GF 组的边缘适合性有显著变化。
尽管自粘接流动树脂复合材料的边缘适合性与高填充流动树脂复合材料和传统流动树脂复合材料相比略差,但经过 24 个月后,修复后的牙齿表现出可接受的临床性能。