Suppr超能文献

不同类型氟化物对不同钛基弓丝拉伸性能和表面粗糙度影响的评估:一项研究。

Evaluation of the Effect of Different Types of Fluoride on Tensile Properties and Surface Roughness of Different Titanium-Based Archwires: An Study.

作者信息

Balakrishnan Rajkumar, Jeri Sumaya Yousuf, Rekha V R, Singh Gangesh Bahadur, Deepak P R, Nair Achuthan

机构信息

Department of Orthodontics, Vivekananda Dental College and Hospital, Thiruchengodu, Tamil Nadu, India.

Department of Orthodontics and Dentofacial Orthopedics, ITS-CDSR, Muradnagar Ghaziabad, Uttar Pradesh, India.

出版信息

J Pharm Bioallied Sci. 2021 Nov;13(Suppl 2):S1193-S1198. doi: 10.4103/jpbs.jpbs_341_21. Epub 2021 Nov 10.

Abstract

OBJECTIVES

The purpose of the study was to evaluate the effect of different types of fluoride on tensile properties and surface roughness of titanium based archwires clinically.

MATERIALS AND METHODS

Three groups of archwires, namely nickel-titanium (NiTi), heat activated NiTi, and TMA was evaluated clinically. Each group comprised four subgroups, namely as received group, nonfluoride control group, APF gel group (received one application of 1.23% APF gel), and sodium fluoride mouthwash group (patients rinsed twice daily with 0.2% sodium fluoride mouthwash). All the archwires were removed after 3 weeks of clinical use and evaluated for surface roughness with three dimensional optical profiler. Tensile strength and elongation rate was determined with Instron universal testing machine.

RESULTS

NiTi, heat activated NiTi, and TMA archwires with APF gel application showed the highest reduction in tensile strength and elongation rate and highest value for surface roughness, followed by sodium fluoride mouthwash group and finally wires without fluoride application. NiTi wires had the highest reduction in tensile strength with APF gel followed by heat activated NiTi and TMA.

CONCLUSION

APF gel with highest concentration of fluoride caused most degradation in the tensile properties and surface roughness of titanium based arch wires.

摘要

目的

本研究的目的是在临床上评估不同类型的氟化物对钛基弓丝拉伸性能和表面粗糙度的影响。

材料与方法

临床上评估了三组弓丝,即镍钛(NiTi)弓丝、热激活镍钛弓丝和TMA弓丝。每组包括四个亚组,即接收组、无氟对照组、APF凝胶组(接受一次1.23%APF凝胶处理)和氟化钠漱口水组(患者每天用0.2%氟化钠漱口水漱口两次)。临床使用3周后取出所有弓丝,用三维光学轮廓仪评估表面粗糙度。用Instron万能试验机测定拉伸强度和伸长率。

结果

应用APF凝胶的NiTi弓丝、热激活镍钛弓丝和TMA弓丝的拉伸强度和伸长率降低幅度最大,表面粗糙度值最高,其次是氟化钠漱口水组,最后是未使用氟化物的弓丝。APF凝胶处理后,NiTi弓丝的拉伸强度降低幅度最大,其次是热激活镍钛弓丝和TMA弓丝。

结论

氟化物浓度最高的APF凝胶对钛基弓丝的拉伸性能和表面粗糙度造成的降解最大。

相似文献

本文引用的文献

1
Mechanical properties and surface characteristics of three archwire alloys.三种弓丝合金的力学性能和表面特征
Angle Orthod. 2004 Dec;74(6):825-31. doi: 10.1043/0003-3219(2004)074<0825:MPASCO>2.0.CO;2.