Suppr超能文献

两种含甲基丙烯酸甲酯-三丁基硼的水基黏结剂联合硅烷-膦酸酯处理剂对 4 种不同 CAD/CAM 树脂复合材料黏结效果的影响。

Effects of two methyl methacrylate-tributylborane-based luting agents with a silane-phosphate primer on bonding of four different CAD/CAM resin composite materials.

机构信息

Division of Cariology and Restorative Dentistry, Department of Prosthetic Dentistry, Graduate School of Biomedical Sciences, Nagasaki University.

出版信息

J Oral Sci. 2022;64(2):167-171. doi: 10.2334/josnusd.21-0513.

Abstract

PURPOSE

This study compared the bond strengths of four adhesive systems and four different resin composite block materials: Gradia Block (GR), Shofu Block HC (SH), Estelite Block (ES), and KZR-CAD HR2 (KZ).

METHODS

A primer (PZ-AB) containing a silane (γ-MPTS) with 10-methacryloyloxydecyl dihydrogen phosphate (MDP) was applied to ground surfaces of the resin composite block specimens, and the specimens were then bonded to stainless-steel rods using two methyl methacrylate-tributylborane (MMA-TBB)-based luting agents (SB and MT), designated as the PZ-AB/SB and PZ-AB/MT adhesive systems, respectively. The SB resin contained 4-methacryloyloxyethyl trimellitate anhydride (4-META), whereas the MT resin did not. The SB resin without primer (No primer/SB) and a dual-curing composite-type adhesive system (UPA/RelyX) were used as controls. The 24-h tensile bond strengths were determined and analyzed using the Tukey-Kramer HSD test (α = 0.05, n = 8).

RESULTS

The highest bond strengths were obtained for the GR/PZ-AB/MT, GR/PZ-AB/SB, KZ/PZ-AB/MT, ES/PZ-AB/SB, and KZ/No primer/SB groups, whereas the KZ/UPA/RelyX, ES/UPA/RelyX, SH/UPA/RelyX, and SH/No primer/SB groups exhibited the lowest bond strengths.

CONCLUSION

For each resin composite block material primed with γ-MPTS and MDP, the MMA-TBB-based luting agents, irrespective of the presence of 4-META, provided higher bond strengths than the dual-curing composite-type adhesive system.

摘要

目的

本研究比较了四种黏接系统和四种不同的树脂复合块材料的黏接强度:Gradia Block(GR)、Shofu Block HC(SH)、Estelite Block(ES)和 KZR-CAD HR2(KZ)。

方法

将含有硅烷(γ-MPTS)和 10-甲氧基丙烯酰氧癸基二氢磷酸酯(MDP)的底漆(PZ-AB)应用于树脂复合块试件的研磨面,然后使用两种甲基丙烯酸甲酯-三丁基硼烷(MMA-TBB)基黏结剂(SB 和 MT)将试件黏接到不锈钢棒上,分别命名为 PZ-AB/SB 和 PZ-AB/MT 黏接系统。SB 树脂含有 4-甲氧基丙烯酰氧乙基偏苯三酸酐(4-META),而 MT 树脂则不含。无底漆的 SB 树脂(No primer/SB)和双固化复合黏接剂系统(UPA/RelyX)被用作对照。采用 Tukey-Kramer HSD 检验(α=0.05,n=8)对 24 h 拉伸黏接强度进行了测定和分析。

结果

GR/PZ-AB/MT、GR/PZ-AB/SB、KZ/PZ-AB/MT、ES/PZ-AB/SB 和 KZ/No primer/SB 组的黏接强度最高,而 KZ/UPA/RelyX、ES/UPA/RelyX、SH/UPA/RelyX 和 SH/No primer/SB 组的黏接强度最低。

结论

对于用 γ-MPTS 和 MDP 预处理的每种树脂复合块材料,基于 MMA-TBB 的黏结剂,无论是否含有 4-META,其黏接强度均高于双固化复合黏接剂系统。

文献检索