Ogata Yudai, Kawaguchi Daisuke, Yamada Norifumi L, Tanaka Keiji
Neutron Science Laboratory, High Energy Accelerator Research Organization, Ibaraki 319-1106, Japan.
International Institute for Carbon-Neutral Energy Research (WPI-I2CNER), Kyushu University, Fukuoka 819-0395, Japan.
ACS Macro Lett. 2013 Oct 15;2(10):856-859. doi: 10.1021/mz400322q. Epub 2013 Sep 13.
Water sorption kinetics in thin Nafion films prepared on silver and silicon oxide substrates was examined by surface plasmon resonance and neutron reflectivity measurements. It was found that the films thickened in three regimes. The asymptotic swelling ratios in regimes I, II, and III were 1.05, 1.26, and 1.41, respectively. These values were independent of the substrate species and were coincident with the transition points of different hydration states in the bulk Nafion; water binding to sulfonic acid groups, the formation of sphere-like ionic clusters, and bridge formation between clusters. The swelling was much slower in thin films than in the bulk due to the mobility restriction of Nafion near the substrate.
通过表面等离子体共振和中子反射率测量,研究了在银和氧化硅衬底上制备的薄Nafion膜中的水吸附动力学。发现这些膜在三个阶段增厚。阶段I、II和III中的渐近溶胀比分别为1.05、1.26和1.41。这些值与衬底种类无关,并且与本体Nafion中不同水合状态的转变点一致;水与磺酸基团结合、形成球状离子簇以及簇之间形成桥。由于衬底附近Nafion的迁移限制,薄膜中的溶胀比本体中的慢得多。