Chen Wei, Wang Chunyu, Yao Xiao, Song Weikai, Zou Yiwei
College of Materials Science & Engineering, Nanjing Tech University, Nanjing 211816, China.
COSL Oilfield Chemicals R&D Institute, Sanhe 065200, China.
ACS Omega. 2024 Feb 15;9(8):9090-9097. doi: 10.1021/acsomega.3c07890. eCollection 2024 Feb 27.
The fluid loss additive is to prevent the cement slurry from filtrating water to the formation under pressure. 2-Acrylamido-2-methylpropanesulfonic acid (AMPS)-based fluid loss additive mainly works by adsorbing on the surface of cement particles. The adsorption affects cement hydration. In this paper, the effect of one kind of AMPS-based fluid loss additive (A-FLA) on the hydration of oil well cement was studied. The water loss, setting time, thickening time, and compressive strength of cement slurry with various amounts of FLA were measured. In addition, the hydration heat of the cement slurry, FLA adsorption isotherm on cement particles, and hydration minerals were studied. The results showed that A-FLA had a good water loss control ability. The water loss of the cement slurry decreased slowly with the increase of A-FLA dosage when the adsorption capacity exceeded 4.47 mg/g. The low adsorption capacity of A-FLA (less than 4.47 mg/g) had a significant impact on the thickening time. With an adsorption capacity greater than 4.47 mg/g, the thickening time varied minimally. A-FLA mainly delayed the hydration of CS at 1 day and reduced the production amorphous phase.
降滤失添加剂用于防止水泥浆在压力下向地层滤失水分。基于2-丙烯酰胺基-2-甲基丙磺酸(AMPS)的降滤失添加剂主要通过吸附在水泥颗粒表面起作用。这种吸附会影响水泥水化。本文研究了一种基于AMPS的降滤失添加剂(A-FLA)对油井水泥水化的影响。测量了含有不同用量FLA的水泥浆的失水量、凝结时间、稠化时间和抗压强度。此外,还研究了水泥浆的水化热、FLA在水泥颗粒上的吸附等温线以及水化矿物。结果表明,A-FLA具有良好的降滤失能力。当吸附量超过4.47mg/g时,水泥浆的失水量随A-FLA用量的增加而缓慢降低。A-FLA的低吸附量(小于4.47mg/g)对稠化时间有显著影响。当吸附量大于4.47mg/g时,稠化时间变化最小。A-FLA主要在1天时延缓了CS的水化,并减少了非晶相的生成。