Jathan Kyathi K, Gaikwad Ajay Kumar, Sanyal Pronob
Prosthodontics and Crown & Bridge, Krishna Vishwa Vidyapeeth, Malkapur, IND.
Cureus. 2024 Jul 16;16(7):e64699. doi: 10.7759/cureus.64699. eCollection 2024 Jul.
The study aims to assess the effect of surface treatments by chemical agents on the retentive strengths of crowns fabricated from polymethylmethacrylate (PMMA) reinforced with graphene nanoparticles adhesively bonded to abutments after thermocycling.
In vitro comparative study.
This study is composed of four groups - one control, one treated with 99% pure etchant acetone solution, one treated with 15 wt% potassium hydrogen fluoride solution, and the last group treated with a combination of both solutions.
The results showed that the mean load in Group A is 228.46±3.16, Group B is 252.57±7.14, Group C is 184.51±6.61, and Group D is 211.03±2.54. The mean score is highest for Group B followed by Group A and Group D, and it is least for Group C. One-way analysis of variance (ANOVA) detected highly significant differences (p<0.01) among the four groups.
It can be concluded that acetone is the best chemical etchant solution for crowns fabricated from G-CAM discs (Graphenano Dental, Graphenano Nanotechnologies, Spain).
本研究旨在评估化学试剂表面处理对热循环后通过纳米石墨烯颗粒增强的聚甲基丙烯酸甲酯(PMMA)制作的冠粘结于基牙后的固位强度的影响。
体外对照研究。
本研究分为四组——一组为对照组,一组用99%纯蚀刻剂丙酮溶液处理,一组用15 wt%氟化氢钾溶液处理,最后一组用两种溶液联合处理。
结果显示,A组的平均载荷为228.46±3.16,B组为252.57±7.14,C组为184.51±6.61,D组为211.03±2.54。平均分最高的是B组,其次是A组和D组,最低的是C组。单因素方差分析(ANOVA)检测到四组之间存在高度显著差异(p<0.01)。
可以得出结论,丙酮是用于由G-CAM盘(Graphenano Dental,Graphenano Nanotechnologies,西班牙)制作的冠的最佳化学蚀刻剂溶液。