Abstract

BACKGROUND

Indirect restorations are a staple restorative option in dentistry due to their versatility, exceptional aesthetics, and desirable strength and longevity. Metal ceramics and all ceramics are the material of choice for permanent restorations but come with certain disadvantages, such as chipping, fracture, and wear of the antagonist tooth or restoration. Polymethylmethacrylate (PMMA) and indirect composite resins are commonly used materials due to their favourable properties for temporary restorations, but lately, they have been chosen as the restorative material of choice for implant-supported full-mouth rehabilitations. This study aimed to evaluate and compare the colour stability and surface roughness of PMMA and indirect composite resins under both ageing and non-ageing conditions. This would greatly help a clinician in choosing materials depending on the clinical scenarios.

AIM

This study aims to evaluate the colour stability and surface roughness of PMMA and indirect composite resins with and without ageing.

METHODS

Specimens of PMMA and indirect composite resins were fabricated and subjected to an ageing process involving thermocycling in the TW-C4.4 (Tae-Won Tech, Incheon, Korea) and immersion in a staining solution. Colour stability was assessed using a spectrophotometer (SpectraMagic NX, RM2002QC, Konica Minolta Corp., Ramsey, Japan), and surface roughness was measured using a stylus profilometer (Mituyoto, Mituyoto Corporation, Kawasaki, Japan). Statistical analysis was performed using IBM SPSS Statistics for Windows, Version 24 (Released 2016; IBM Corp., Armonk, New York) to determine significant differences between materials and ageing effects.

RESULTS

PMMA exhibited significantly higher colour changes and increased surface roughness post-ageing compared to indirect composite resins. The findings underscored PMMA's susceptibility to discolouration and surface degradation under thermal stress conditions.

CONCLUSION

PMMA demonstrates inferior colour stability and increased surface roughness following thermocycling compared to indirect composite materials, suggesting careful consideration in material selection for provisional restorations. Further research should explore additional ageing processes and materials to enhance understanding and improve clinical outcomes.

摘要

背景

间接修复体因其多功能性、出色的美观性以及理想的强度和耐久性,成为牙科领域常用的修复选择。金属陶瓷和全陶瓷是永久修复体的首选材料,但存在一些缺点,如崩瓷、折断以及对颌牙或修复体的磨损。聚甲基丙烯酸甲酯(PMMA)和间接复合树脂因其适用于临时修复体的良好性能而被广泛使用,但最近,它们已被选为种植体支持的全口修复的修复材料。本研究旨在评估和比较PMMA和间接复合树脂在老化和非老化条件下的颜色稳定性和表面粗糙度。这将极大地帮助临床医生根据临床情况选择材料。

目的

本研究旨在评估老化和未老化条件下PMMA和间接复合树脂的颜色稳定性和表面粗糙度。

方法

制作PMMA和间接复合树脂标本,并进行老化处理,包括在TW-C4.4(韩国仁川太元科技公司)中进行热循环以及浸泡在染色溶液中。使用分光光度计(SpectraMagic NX,RM2002QC,日本柯尼卡美能达公司,拉姆齐)评估颜色稳定性,并使用触针式轮廓仪(Mituyoto,日本三丰公司,川崎)测量表面粗糙度。使用IBM SPSS Statistics for Windows,版本24(2016年发布;IBM公司,纽约州阿蒙克)进行统计分析,以确定材料之间以及老化效应的显著差异。

结果

与间接复合树脂相比,PMMA在老化后表现出显著更高的颜色变化和表面粗糙度增加。研究结果强调了PMMA在热应力条件下易变色和表面降解的特性。

结论

与间接复合材料相比,PMMA在热循环后表现出较差的颜色稳定性和增加的表面粗糙度,这表明在临时修复体的材料选择中应谨慎考虑。进一步的研究应探索其他老化过程和材料,以增进理解并改善临床结果。

https://cdn.ncbi.nlm.nih.gov/pmc/blobs/c83d/11438527/f8361af3798d/cureus-0016-00000068073-i01.jpg

文献AI研究员

20分钟写一篇综述,助力文献阅读效率提升50倍。

立即体验

用中文搜PubMed

大模型驱动的PubMed中文搜索引擎

马上搜索

文档翻译

学术文献翻译模型,支持多种主流文档格式。

立即体验