Suppr超能文献

两种根管封闭剂(或联合牙胶)的侧向加压充填技术对根管治疗后牙疲劳性能和破坏模式的影响。

The impact of the filling technique with two sealers in bulk or associated with gutta-percha on the fatigue behavior and failure patterns of endodontically treated teeth.

机构信息

Post-Graduate Program in Oral Science, Universidade Federal de Santa Maria, Santa Maria, Rio Grande do Sul, Brazil.

Faculty of Dentistry, Universidade Federal de Santa Maria, Santa Maria, Rio Grande do Sul, Brazil.

出版信息

PeerJ. 2024 Oct 28;12:e18221. doi: 10.7717/peerj.18221. eCollection 2024.

Abstract

BACKGROUND

The present study aimed to evaluate the fatigue behavior of teeth filled with a calcium silicate-based sealer (Bio-C Sealer, BC) or an epoxy resin-based sealer (AH Plus, AH), in bulk or associated with gutta-percha as main core material.

METHODS

Seventy-two sound human maxillary anterior teeth were initially selected. Sixty of them, were randomly chosen, and had their root canals prepared using nickel-titanium reciprocating instruments, being again randomly assigned to five experimental groups ( = 12): C+ (control + prepared but not filled); BC-B (BC in bulk); BC-GP (BC+ gutta-percha); AP-B (AH in bulk); AP-GP (AH+ gutta-percha). An additional negative control group (C-) was considered ( = 12), consisting only on sound teeth, without preparation and filling. The specimens were submitted to a survival analysis after the cyclic fatigue test.

RESULTS

Sound teeth (C-) presented the best fatigue performance ( < 0.05), being similar only to the AP-GP group ( > 0.05). Despite that, all experimental groups showed similar fatigue behavior ( > 0.05) to C+ (BC-B = BC-GP = AP-B = AP-GP = C+). Based on that, it can be seen that the use of gutta-percha, as a main core material, associated with the AH Plus sealer, reestablished the mechanical fatigue performance of endodontically treated teeth comparable to sound teeth, still consisting on the most promising approach to rehabilitate such scenario. Teeth filled in bulk, had discreetly higher risk of premature failures and inferior fatigue performance.

摘要

背景

本研究旨在评估以硅酸钙为基础的密封剂(Bio-C Sealer,BC)或环氧树脂为基础的密封剂(AH Plus,AH)在整体或与牙胶作为主要核心材料联合使用时对牙齿的疲劳性能。

方法

最初选择了 72 颗健康的上颌前牙。其中 60 颗随机选择,并使用镍钛往复器械预备根管,然后再次随机分配到五个实验组(每组 12 颗):C+(对照+预备但未填充);BC-B(BC 整体填充);BC-GP(BC+牙胶);AP-B(AH 整体填充);AP-GP(AH+牙胶)。还考虑了一个阴性对照组(C-)(每组 12 颗),仅由未预备和未填充的健康牙齿组成。循环疲劳试验后,对标本进行生存分析。

结果

健康牙齿(C-)表现出最佳的疲劳性能(<0.05),仅与 AP-GP 组相似(>0.05)。尽管如此,所有实验组的疲劳行为与 C+(BC-B=BC-GP=AP-B=AP-GP=C+)相似(>0.05)。基于此,可以看出,牙胶作为主要核心材料与 AH Plus 密封剂联合使用,恢复了根管治疗后牙齿的机械疲劳性能,使其与健康牙齿相当,仍然是修复这种情况的最有前途的方法。整体填充的牙齿有更高的早期失效风险和较差的疲劳性能。