Oshika Miyuki, Kishimoto Takafumi, Horie Taku, Alhotan Abdulaziz, Irie Masao, Sule Veronica C, Barkmeier Wayne W, Tsujimoto Akimasa
Department of Operative Dentistry, School of Dentistry, Aichi Gakuin University, Nagoya 464-8651, Japan.
Department of Oral Health Sciences, BIOMAT, KU Leuven, 3000 Leuven, Belgium.
J Funct Biomater. 2024 Dec 26;16(1):5. doi: 10.3390/jfb16010005.
The purpose of this study was to compare the wear resistance of light-cure resin luting cements for veneers with that of other luting materials investigated in earlier studies. An Alabama wear-testing machine was used to measure the wear resistance of four recent light-cure resin luting cements for veneers (G-Cem Veneer; Panavia V5 LC; RelyX Veneer Cement; and Vario-link Esthetic LC). The volume loss ranged from 0.027 ± 0.003 to 0.119 ± 0.030 mm, the mean facet depth from 56.053 ± 7.074 to 81.531 ± 7.712 µm, and the maximum facet depth from 100.439 ± 26.534 to 215.958 ± 27.320 µm. G-Cem Veneer showed significantly better ( < 0.05) wear resistance than the other materials tested. Representative SEM images were obtained which showed differences in form among the wear facets for the luting cements examined. Correlations were calculated between the three measurements for each material, and the pattern of correlations was also different for each material.
本研究的目的是比较用于贴面的光固化树脂粘结水门汀与早期研究中所调查的其他粘结材料的耐磨性。使用阿拉巴马磨损试验机测量了四种用于贴面的近期光固化树脂粘结水门汀(G-Cem Veneer;Panavia V5 LC;RelyX Veneer Cement;以及Vario-link Esthetic LC)的耐磨性。体积损失范围为0.027±0.003至0.119±0.030毫米,平均刻面深度为56.053±7.074至81.531±7.712微米,最大刻面深度为100.439±26.534至215.958±27.320微米。G-Cem Veneer的耐磨性显著优于(<0.05)其他测试材料。获得了代表性的扫描电子显微镜图像,这些图像显示了所检查的粘结水门汀磨损刻面在形态上的差异。计算了每种材料的三项测量值之间的相关性,并且每种材料的相关模式也不同。